Macromolecule anticorrosion paint and preparing method thereof

An anti-corrosion coating and polymer technology, applied in anti-corrosion coatings, wax coatings, natural rubber coatings, etc., can solve the problems of high construction requirements, unusable, large volume, etc., and achieve scientific and reasonable preparation methods, high acid and alkali resistance, The effect of high surface density
CN101012348AInactive Publication Date: 2007-08-08包洪钧

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
包洪钧
Publication Date
2007-08-08
Estimated Expiration
Not applicable · inactive patent
Patent Text Reader

Abstract

The invention discloses a macromolecular preservative paint and preparing method, which comprises the following steps: allocating raw material with 55% filming material, 11% solvent, 11% paint adjuvant and 23% dye and fill; heating filming material to dissolve; stirring to add emulsion to emulsify; adding solvent, paint adjuvant to grind; beating; stirring; filtering; detecting viscosity; selecting filming material from oil-water amphiprotic acrylic acid resin, natural rubber, chlorcosane and zinc stearic acid; making isopropanol as solvent.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to a paint and a preparation method thereof, more specifically to a polymer anticorrosion paint with acrylic resin as the main film-forming substance and a preparation method thereof. Background technique

[0002] Coating is a kind of chemical product with convenient construction, low price, obvious effect and high added value rate. It not only has the function of preventing the surface of buildings, ships, machinery, etc. Strong fine chemical product.

[0003] The existing widely used anti-corrosion fluorocarbon paint has good anti-corrosion properties, but it has the following problems:

[0004] Problem 1: High construction requirements. It needs to be composed of A and B pairs, and it is prepared and used at the construction site. The construction is limited by time and must be used within 10 hours, otherwise it cannot be used after curing.

[0005] Question 2: For steel structures, the requirements for anti-corrosion surfa...

Claims