A technology of low-concentration heavy metals and microbial methods, which is applied in water/sewage treatment, anaerobic digestion treatment, process efficiency improvement, etc., can solve the problems that do not involve heavy metal separation and recovery, and the concentration of heavy metal ions is not too high, so as to achieve good industrial application Prospect, the effect of high recovery rate of valuable metal ions and low treatment cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0024] The concentrations of metal ions in the biometallurgical leaching solution to be processed (nickel pyrite leaching solution) are:
[0025] Fe 3+ :5g / L, Ni 2+ :2g / L, Cu 2+ :0.5g / L, Mg 2+ :20g / L
[0026] When the two units of acid-producing fermentation and hydrogen sulfide production by sulfate-reducing bacteria are successfully started and operating stably, and the total sulfide output continues to stabilize above about 300 mg / L, the outlet liquid in the reactor is injected into the precipitation reactor . Among them, the hydrogen sulfide production reactor of sulfate-reducing bacteria is filled with porcelain rings as an immobilization carrier. Cu 2+ The sulfide precipitate is formed first, and almost completely precipitates when the pH value is 1 to 3. The Cu finally detected in the treated leachate 2+ Content is less than 5mg; adjust pH value, Fe 3+ And Ni 2+ When the pH value is 2~8, it will gradually transform into sulfide precipitation, and the final Fe detected in th...
Embodiment 2
[0028] The concentrations of metal ions in the biometallurgical leaching solution to be processed (nickel pyrite leaching solution) are:
[0029] Fe 3+ :5g / L, Ni 2+ :2g / L, Cu 2+ :0.5g / L, Mg 2+ :20g / L
[0030] When the two units of acid-producing fermentation and hydrogen sulfide production by sulfate-reducing bacteria are successfully started and operating stably, and the total sulfide output continues to stabilize above about 300 mg / L, the outlet liquid in the reactor is injected into the precipitation reactor . The hydrogen sulfide production reactor of sulfate-reducing bacteria is filled with sponge as an immobilized carrier. Cu 2+ The sulfide precipitate is formed first, and almost completely precipitates when the pH value is 1 to 3. The Cu finally detected in the treated leachate 2+ Content is less than 2mg; adjust pH value, Fe 3+ And Ni 2+ When the pH value is 2~8, it will gradually transform into sulfide precipitation, and the final Fe detected in the solution after precipi...
Embodiment 3
[0032] The concentrations of metal ions in the biometallurgical leaching solution (copper sulfide ore leaching tailings) to be processed are:
[0033] Fe 3+ :5g / L, Cu 2+ :10g / L
[0034] The specific implementation method is the same as in Example 1, Cu 2+ First, sulfide precipitates are formed, and they are almost completely precipitated when the pH is 1 to 3. The Cu finally detected in the leaching solution after treatment 2+ The content is less than 50mg; adjust the pH value, Fe 3+ When the pH value is 2~9, it will gradually transform into sulfide precipitation, and the final Fe detected in the leachate after precipitation 3+ The content is less than 12mg, and the valuable metals have a higher recovery rate, 99% for copper and 95% for iron.