Aluminium zinc phosphomolybdate compounded rustproof pigment and production method thereof
A technology of anti-rust pigments and aluminum phosphomolybdate, which is applied in the direction of phosphorus compounds, pigment pastes, anti-corrosion coatings, etc., can solve the problem of anti-rust pigments such as aluminum-zinc phosphomolybdate, iron red, zinc phosphate and modified phosphoric acid. Zinc, aluminum tripolyphosphate, zinc phosphomolybdate series, ion exchange pigments, magnesium ferrite and phosphite, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] Add water to the stirring paddle in the reaction kettle, heat it to 55°C, and then add 120 kg of aluminum zinc phosphate, 20 kg of aluminum phosphate and 2 kg of zinc aluminate under stirring. After 30 minutes, add 15 kilograms of barium sulfate and 15 kilograms of zinc oxide, and continue to react for 30 minutes. After the temperature drops to 40 ° C, add 0.2 kilograms of diethanolamine, start high-speed stirring, and control 200 rpm. Centrifugal dehydration, drying, crushing, weighing, and packaging into products.
Embodiment 2
[0029] Add water to the stirring paddle in the reaction kettle, heat to 80°C, and then add 140 kg of aluminum zinc phosphate, 35 kg of aluminum phosphate and 8 kg of zinc molybdate under stirring. After 30 minutes, add 3 kilograms of barium sulfate and 10 kilograms of zinc oxide, and continue to react for 30 minutes. After the temperature drops to 35 ° C, add 1 kilogram of triethanolamine, start high-speed stirring, and control 250 rpm. Centrifugal dehydration, drying, crushing, weighing, and packaging into products.
Embodiment 3
[0031] Add water to the reactor to the stirring paddle, heat to 95°C, and then add 100 kg of aluminum zinc phosphate, 40 kg of aluminum phosphate and 1 kg of zinc aluminate under stirring. After 30 minutes, add 2 kilograms of barium sulfate and 6 kilograms of zinc oxide, and continue to react for 30 minutes. After the temperature drops to 50 ° C, add 0.5 kilograms of monoethanolamine, start high-speed stirring, and control 350 rpm. Centrifugal dehydration, drying, crushing, weighing, and packaging into products.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com