Engine lubricating oil filtering material and production technique thereof
A technology of filter material and production process, which is applied in the direction of engine lubrication, engine components, machine/engine, etc., can solve the problems of wasting wood resources, destroying ecological balance, and poor filtering effect, so as to achieve good filtering effect, save energy and prolong The effect of service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] A. Production of bamboo fiber:
[0018] Take the adult bamboo (3-5 years old) Hsinchu, remove the branches and leaves, use a wire drawing machine to draw bamboo wires with a diameter of 0.6-1mm, then cut them into 3-5mm long bamboo wires with a cutting machine, put the bamboo wires into the softening solution Among them, the softening solution is prepared by mixing 4% sodium hydroxide, 3% sodium sulfite, 15% sodium sulfate, and the rest of water by weight percentage, soaked for 34 hours, and then cooked at 80°C for 2.5 hours Wash with clear water, dry or sun-dry when measuring pH value 6-8, when making water content 15%, make the bamboo fiber that diameter is 0.08-0.2mm with loosening machine repeatedly;
[0019] B. Production of hemp fiber:
[0020] Soak the hemp in 8% sodium hydroxide solution by mass for 75 hours, rinse it with water, dry it when the pH value is 6-9 or dry it naturally, cut it into 3-5mm segments, and loosen it. The machine repeatedly sorts into fl...
Embodiment 2
[0024] A. Production of bamboo fiber:
[0025] Take the adult bamboo (3-5 years old) Hsinchu, remove the branches and leaves, use a wire drawing machine to draw bamboo wires with a diameter of 0.6-1mm, then cut them into 3-5mm long bamboo wires with a cutting machine, put the bamboo wires into the softening solution In this method, the softening solution is prepared by mixing 6% sodium hydroxide, 1% sodium sulfite, 13% sodium sulfate, and the rest of water by weight percentage, soaked for 38 hours, and then cooked at 100 ° C for 1.5 hours Wash with clear water, dry or sun-dry when the pH value is 6-8, make the water content 20%, and repeatedly sort out with a loosening machine to make bamboo fibers with a diameter of 0.08-0.2mm;
[0026] B. Production of hemp fiber:
[0027] Soak apocynum in 12% sodium hydroxide solution for 70 hours, rinse with clean water, dry or dry naturally when the pH value is 6-9, cut into 3-5mm line segments, and loosen The machine repeatedly sorts i...
Embodiment 3
[0031] A. Production of bamboo fiber:
[0032] Take the adult bamboo (3-5 years old) Hsinchu, remove the branches and leaves, use a wire drawing machine to draw bamboo wires with a diameter of 0.6-1mm, then cut them into 3-5mm long bamboo wires with a cutting machine, put the bamboo wires into the softening solution In this method, the softening solution is prepared by mixing 5% sodium hydroxide, 2% sodium sulfite, 14% sodium sulfate, and the rest of water by weight percentage, soaked for 36 hours, and then steamed for 2 hours at a temperature of 90°C Wash with clear water, dry or sun-dry when the pH value is 6-8, make the water content 18%, and repeatedly sort out with a loosening machine to make bamboo fibers with a diameter of 0.08-0.2mm;
[0033] B. Production of hemp fiber:
[0034] Soak the flax in 10% sodium hydroxide solution by mass for 72 hours, rinse it with clean water, dry it when the pH value is 6-9 or dry it naturally, cut it into 3-5mm line segments, and pass ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com