A technology of chitosan derivatives and nanocomposites, which is applied in the direction of drug combinations, inorganic active ingredients, and medical preparations of non-effective ingredients. It can solve the problems of preparation methods and applications that have not been reported, and achieve the effect of uniform particle size.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0054] A kind of silver, chitosan nanocomposite, preparation method step is as follows:
[0055] (1) Grind 10g chitosan into fine powder;
[0056] (2) Grinding 0.005g of silver nitrate into fine powder;
[0057] (3) Mix chitosan fine powder and silver nitrate fine powder, and grind thoroughly for 1 hour;
[0058] (4) Add 0.005 g of ascorbic acid, and continue to fully grind for 2 hours to obtain a silver-chitosan nanocomposite (sample 1) with a silver particle size of 1-100 nm.
Embodiment 2
[0060] A nanocomposite of silver and chitosan derivatives, the preparation method steps are as follows:
[0061] (1) Grinding 10g carboxymethyl chitosan into fine powder;
[0062] (2) Grinding 0.005g of silver nitrate into fine powder;
[0063] (3) Mix carboxymethyl chitosan fine powder with silver nitrate fine powder and grind them thoroughly for 2 hours;
[0064] (4) Add 0.005 g of glucose and continue to grind thoroughly for 2.5 hours to obtain a silver-chitosan derivative nanocomposite (sample 2) with a silver particle size of 1-100 nm.
Embodiment 3
[0066] A nanocomposite of silver, chitosan and chitosan derivatives, the preparation method steps are as follows:
[0067] (1) Grind 7g chitosan and 3g hydroxypropyl chitosan into fine powder;
[0068] (2) Grinding 0.005g of silver nitrate into fine powder;
[0069] (3) Mix chitosan and hydroxypropyl chitosan fine powder with silver nitrate fine powder, and fully grind for 2 hours;
[0070] (4) Add 0.005 g of N-acetylglucosamine, and continue to fully grind for 6 hours to obtain silver, chitosan and chitosan derivative nanocomposites with a silver particle size of 1-100 nm.
PUM
Property | Measurement | Unit |
---|---|---|
Particle size | aaaaa | aaaaa |
Concentration | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com