Embodiment 1
[0026] Embodiment 1: The raw material and weight percent of the flocculant of the present embodiment are as follows:
[0027] Fly ash 45%;
[0028] VCM mixed acid (in the process of producing polyvinyl chloride, black waste acid is obtained after drying acetylene and hydrogen chloride gas with concentrated sulfuric acid. Among them, the mass percentage concentration of sulfuric acid is 80-93%, and the mass percentage concentration of hydrochloric acid is 0.5%-2%) 11.5 %;
[0029] Water 43.5%.
[0030] The production technique of flocculant of the present invention, concrete steps are as follows:
[0031] (1) Crushed fly ash
[0032] Take a certain amount of fly ash and pulverize it in a pulverizer, and the powder particles can pass through a 20-mesh sieve.
[0033] (2) Mixed ingredients
[0034] According to the percentage content of each component, weigh the fly ash powder, VCM mixed acid, and water for mixing and stirring. At this time, the pH value of the material is i...
Embodiment 2
[0043] Embodiment 2: The main raw material and weight percentage of the flocculant of the present embodiment are as follows:
[0044] Fly ash 51%;
[0045] VCM mixed acid (the mass percentage concentration of sulfuric acid is 80-93%, the mass percentage concentration of hydrochloric acid is 0.5%-2%) 12%;
[0046] Water 37%.
[0047] The production method of the flocculant of the present embodiment, concrete steps are as follows:
[0048] (1) Crushed fly ash
[0049] Take a certain amount of fly ash and pulverize it in a pulverizer, and the powder particles can pass through a 20-mesh sieve.
[0050] (2) Mixed ingredients
[0051] According to the percentage content of each component, weigh the fly ash powder, VCM mixed acid, and water for mixing and stirring. At this time, the pH value of the material is in the range of 4-7.
[0052] (3) carry out chemical reaction
[0053] Under normal temperature and pressure, the alumina and iron oxide in the fly ash are fully reacted ...
Embodiment 3
[0060] Embodiment 3: The main raw material and weight percentage of the flocculant of the present embodiment are as follows:
[0061] Fly ash 60%;
[0062] VCM mixed acid (the mass percentage concentration of sulfuric acid is 80-93%, the mass percentage concentration of hydrochloric acid is 0.5%-2%) 18%;
[0063] Water 22%.
[0064] The production technology of the flocculant of the present embodiment, concrete steps are as follows:
[0065] (1) Crushed fly ash
[0066] Take a certain amount of fly ash and pulverize it in a pulverizer, and the powder particles can pass through a 20-mesh sieve.
[0067] (2) Mixed ingredients
[0068] According to the percentage content of each component, weigh the fly ash powder, VCM mixed acid, and water for mixing and stirring. At this time, the pH value of the material is in the range of 4-7.
[0069] (3) carry out chemical reaction
[0070] Under normal temperature and pressure, the alumina and iron oxide in the fly ash are fully reac...