A formaldehyde adsorption and indication technology, applied in separation methods, chemical instruments and methods, and other chemical processes, can solve the problems of secondary pollution, exhaustion, and inability to indicate the life of materials, etc., and achieve the effect of low cost and simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] This embodiment provides an indicating formaldehyde adsorbent, which is prepared through the following steps:
[0022] (1) Mix magnesium hydroxide and alumina monohydrate with a molar ratio of 2:1, add attapulgite with a weight equal to 10% of the total weight of magnesium hydroxide and alumina monohydrate, and appropriate amount of water, mix well, and set aside ;
[0023] (2) Extrude the mixture of step (1) through an extruder to obtain cylindrical particles with a diameter of 0.8mm and a length of 6mm, and then dry the particles at 110°C (moisture content below 5%);
[0024] (3) Prepare a 1wt% potassium permanganate impregnation solution, and use the obtained solution to impregnate the dried particles in step (2). The impregnation temperature is normal temperature, and the impregnation time is 2 hours. The obtained particles were quickly dried (the drying temperature was 85° C.) to obtain a purple-red indicating formaldehyde adsorbent.
Embodiment 2
[0026] This embodiment provides an indicating formaldehyde adsorbent, which is prepared through the following steps:
[0027] (1) Mix magnesium hydroxide and aluminum oxide monohydrate with a molar ratio of 3:1, add bentonite with a weight of 30% of the total weight of magnesium hydroxide and aluminum oxide monohydrate, and appropriate amount of water, mix well, and set ;
[0028] (2) Extrude the mixture of step (1) through an extruder to obtain cylindrical granules with a diameter of 3mm and a length of 8mm, and then dry the granules at 110°C (moisture content below 5 %);
[0029] (3) Prepare a 3wt% sodium permanganate impregnation solution, impregnate the dried particles in step (2) with the prepared solution, impregnate for 1.5 hours, and finally use a potassium permanganate dryer to quickly dry the impregnated particles (Drying temperature is 90°C) to obtain purple-red indicating formaldehyde adsorbent.
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
| length | aaaaa | aaaaa |
| diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More 