A technology of ceiling and PVC resin, applied in the field of ceiling and its preparation, can solve the problems of affecting the appearance of the ceiling, not having dustproof, sound-absorbing, insect-proof and reflective, and not having dust-proof, so as to achieve good sound insulation and heat insulation effect, and improve lighting degree, strong effect of scratch resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] Environmentally friendly PVC foam ceiling board, including the following components in parts by mass: 90 parts of PVC resin; 5 parts of polylactic acid; 7 parts of polycaprolactone; 10 parts of polyester fiber; 50 parts of barium sulfate; 3 parts; 5 parts of zinc stearate; 1.7 parts of titanium dioxide; 0.6 parts of PE wax; 2 parts of ACR-201 processing modifier; 1.4 parts of CPE impact modifier; 0.7 parts of BTH composite foaming agent; sepiolite 20 servings.
[0029] The preparation method of environment-friendly PVC foam ceiling plate comprises the following steps:
[0030] Step 1: Screen the barium sulfate through a 160-mesh screen and add it to the mixer, then add PVC resin, polylactic acid, polycaprolactone, polyester fiber, and mix and stir for 10 minutes;
[0031] Step 2: Then add plasticizer, stabilizer, titanium dioxide, PE wax, processing modifier, impact modifier, composite foaming agent, sepiolite and mix for 20 minutes, cool down to a temperature of ≤45°C...
Embodiment 2
[0035] Environmentally friendly PVC foam ceiling board, including the following components in parts by mass: 110 parts of PVC resin; 10 parts of polylactic acid; 12 parts of polycaprolactone; 20 parts of polyester fiber; 70 parts of barium sulfate; 7 parts; 11 parts of zinc stearate; 5 parts of titanium dioxide; 2 parts of PE wax; 5.5 parts of ACR-201 processing modifier; 3.2 parts of CPE impact modifier; 1.5 parts of BTH composite blowing agent; sepiolite 30 servings.
[0036] The preparation method of environment-friendly PVC foam ceiling plate comprises the following steps:
[0037] Step 1: Screen the barium sulfate through a 200-mesh screen and add it to the mixer, then add PVC resin, polylactic acid, polycaprolactone, polyester fiber, and mix and stir for 15 minutes;
[0038] Step 2: Then add plasticizer, stabilizer, titanium dioxide, PE wax, processing modifier, impact modifier, composite foaming agent, sepiolite and mix for 25 minutes, cool down to a temperature ≤ 45°C...
Embodiment 3
[0042] Environmentally friendly PVC foam ceiling board, including the following components in parts by mass: 93 parts of PVC resin; 5.5 parts of polylactic acid; 7.6 parts of polycaprolactone; 12 parts of polyester fiber; 50 parts of barium sulfate; 3.3 parts; 6 parts zinc stearate; 2.1 parts titanium dioxide; 0.8 parts PE wax; 2.9 parts ACR-201 processing modifier; 1.5 parts CPE impact modifier; 0.8 parts BTH composite blowing agent; sepiolite 21 servings.
[0043] The preparation method of environment-friendly PVC foam ceiling plate comprises the following steps:
[0044] Step 1: Screen the barium sulfate through a 180-mesh screen and add it to the mixer, then add PVC resin, polylactic acid, polycaprolactone, polyester fiber, and mix and stir for 12 minutes;
[0045] Step 2: Then add plasticizer, stabilizer, titanium dioxide, PE wax, processing modifier, impact modifier, composite foaming agent, sepiolite and mix for 22 minutes, cool down to a temperature ≤ 45°C and leave ...
PUM
Property | Measurement | Unit |
---|---|---|
friction coefficient | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com