Smell-purifying inner wall latex paint and preparation method thereof
A technology for interior wall latex paint and odor purification, applied in the field of building decoration materials, can solve the problems of lack of purification of indoor air odor, inability to quickly dissipate irritating odor, etc., and achieve the effect of reducing indoor harmful substances, improving air quality and low VOC
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach
[0033] A clean-odour interior wall latex paint, which is prepared from the following raw materials according to the following mass ratio through the following steps:
[0034] (1) Add 22-28 parts of water into the dispersing tank, add 0.4-0.5 parts of hydroxyethyl cellulose and 0.1-0.3 parts of water-based multifunctional additives in sequence at a speed of 350-550r / min, and disperse for 1-3 minutes;
[0035] (2) After increasing the rotation speed to 800-1000r / min, add 0.5-0.7 parts of water-based dispersant, 0.2-0.3 parts of water-based wetting agent, 0.4-0.5 parts of water-based defoamer, 0.4-0.6 parts of anti-fungal agent, 15 - After 18 parts of titanium dioxide, 8-10 parts of kaolin, 10-15 parts of calcium carbonate, 3-4 parts of diatomaceous earth, 3-4 parts of negative ion pulp and 1-2 parts of imidazolidinone, increase the speed again to 1800-2000r Disperse for 15-20 minutes at a speed of 1 / min, then check whether the fineness is ≤60 μm, if the fineness is ≤60 μm, proce...
Embodiment 1
[0038] Embodiment 1 (best embodiment)
[0039] A clean-odour interior wall latex paint, which is prepared from the following raw materials according to the following mass ratio through the following steps:
[0040] (1) Add 22.2 parts of water into the dispersing tank, add 0.45 parts of hydroxyethyl cellulose and 0.2 parts of water-based multifunctional additives in sequence at 450r / min, and disperse for 2 minutes;
[0041] (2) After increasing the rotation speed to 900r / min, add 0.6 parts of water-based dispersant, 0.2 parts of water-based wetting agent, 0.5 parts of water-based defoamer, 0.4 parts of anti-fungal agent, 16 parts of titanium dioxide, 8 parts of kaolin, 13 parts After calcium carbonate, 4 parts of diatomaceous earth, 3 parts of negative ion slurry and 1.5 parts of imidazolidinone, increase the speed again to 1900r / min and disperse for 18 minutes, then check whether the fineness is ≤60μm, if the fineness is ≤60μm, continue to perform the steps (3);
[0042] (3)...
Embodiment 2
[0044] A clean-odour interior wall latex paint, which is prepared from the following raw materials according to the following mass ratio through the following steps:
[0045] (1) Add 25.85 parts of water into the dispersing tank, add 0.5 parts of hydroxyethyl cellulose and 0.15 parts of water-based multifunctional additives in sequence at a speed of 350r / min, and disperse for 1-3 minutes;
[0046](2) After increasing the rotation speed to 1000r / min, add 0.6 parts of water-based dispersant, 0.3 parts of water-based wetting agent, 0.5 parts of water-based defoamer, 0.5 parts of anti-fungal agent, 15 parts of titanium dioxide, 10 parts of kaolin, 13 parts After calcium carbonate, 3 parts of diatomaceous earth, 2.5 parts of negative ion slurry and 1.5 parts of imidazolidinone, increase the speed again to 1800r / min and disperse for 20 minutes, then check whether the fineness is ≤60μm, if the fineness is ≤60μm, continue to perform the steps (3);
[0047] (3) After reducing the spee...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com