Embodiment 1
[0037] Such as figure 1 and 2 As shown, the street lamp stand includes a base 1, an absorbent concrete outer wall 2, a combination of sawdust activated carbon and titanium dioxide 4; Ventilation holes 3 are evenly arranged on the side, the inside of the air holes is high and the outside is low, and the inclination angle is 45°. The wood chip activated carbon and titanium dioxide combination 4 is placed inside the outer wall of the adsorptive concrete 2; the wood chip activated carbon and titanium dioxide combination 2 is arranged in two adjacent ventilation holes. Between the holes 3, the ventilation holes 3 are located between two adjacent wood chip activated carbon and titanium dioxide assemblies 4, the spacing between each wood chip activated carbon and titanium dioxide assembly 4 is equal, and the spacing between each ventilation hole 3 is equal. The wood chip activated carbon and titanium dioxide combination 4 is a mixture made of wood chip activated carbon and titanium ...
Embodiment 2
[0045] The structure of the street light frame is as in embodiment 1
[0046] A method for processing a street lamp stand for purifying and degrading harmful gases, comprising the following steps:
[0047] The first step: prepare a combination of wood chip activated carbon and titanium dioxide, and mix the wood chip activated carbon and high-titanium heavy slag with a weight content of more than 10% of titanium dioxide at a mass ratio of 2:1 to obtain a mixture; add soda ash and water glass powder to the mixture , soda ash accounts for 2.5% of the total weight of the mixture, water glass powder accounts for 4% of the total weight of the mixture, and evenly mixes to obtain the secondary mixture;
[0048] Mix water glass powder, soda ash and feldspar powder in a mass ratio of 1:2:1.5 to make a low-temperature binder;
[0049] Press the secondary mixture into shape, then add a low-temperature binder, and calcinate at 650°C for 7 hours; use a steel grid frame to package it, and p...
Embodiment 3
[0053] The structure of the street light frame is as in embodiment 1
[0054] A method for processing a street lamp stand for purifying and degrading harmful gases, comprising the following steps:
[0055] The first step: prepare a combination of wood chip activated carbon and titanium dioxide, and mix the wood chip activated carbon and high-titanium heavy slag with a weight content of more than 10% of titanium dioxide at a mass ratio of 2:1 to obtain a mixture; add soda ash and water glass powder to the mixture , soda ash accounts for 2% of the total weight of the mixture, water glass powder accounts for 3% of the total weight of the mixture, and evenly mixes to obtain the secondary mixture;
[0056] Mix water glass powder, soda ash and feldspar powder in a mass ratio of 1:1.5:1.5 to make a low-temperature binder;
[0057] Press the secondary mixture into shape, then add a low-temperature binder, and calcinate at 630°C for 8 hours; use a steel grid to package it, and prepare...