Embodiment 1
[0008] Embodiment 1: a kind of environment-friendly wallpaper base paper is characterized in that being made of the raw material of following mass fraction: 50 parts of bamboo pulp fiber, 10 parts of wood pulp fiber, 15 parts of acrylic fiber, 3 parts of sodium carboxymethyl cellulose 3 parts, 3 parts of nano-bamboo charcoal fiber, 5 parts of inorganic filler, the production steps are: 1) After mixing bamboo pulp fiber and wood pulp fiber, add water with a mass of 100 times, beat with a beater, and control the degree of knocking at 40~ 60° SR, add nano-bamboo charcoal fiber evenly into the mixed pulp 1 to 2 hours after the beating starts, and continue beating to obtain a mixed pulp of bamboo pulp fiber and wood pulp fiber; 2) Add acrylic fiber to 100 times water, beating for 20 to 40 minutes to make acrylic fiber pulp; 3) mixing bamboo pulp fiber, wood pulp fiber mixed pulp and acrylic fiber pulp in the above steps, adding sodium carboxymethyl cellulose and inorganic filler an...
Embodiment 2
[0009] Embodiment 2: a kind of environment-friendly wallpaper base paper is characterized in that being made of the raw material of following mass fraction: 70 parts of bamboo pulp fiber, 25 parts of wood pulp fiber, 25 parts of acrylic fiber, sodium carboxymethyl cellulose 5 parts 7 parts, 7 parts of nano-bamboo charcoal fiber, 15 parts of inorganic filler, the production steps are: 1) After mixing bamboo pulp fiber and wood pulp fiber, add water with a mass of 100 times, and beat with a beater, and the degree of knocking is controlled at 40~ 60° SR, add nano-bamboo charcoal fiber evenly into the mixed pulp 1 to 2 hours after the beating starts, and continue beating to obtain a mixed pulp of bamboo pulp fiber and wood pulp fiber; 2) Add acrylic fiber to 100 times water, beating for 20 to 40 minutes to make acrylic fiber pulp; 3) mixing bamboo pulp fiber, wood pulp fiber mixed pulp and acrylic fiber pulp in the above steps, adding sodium carboxymethyl cellulose and inorganic fi...
Embodiment 3
[0010] Embodiment 3: a kind of environment-friendly wallpaper base paper is characterized in that being made of the raw material of following mass fraction: 60 parts of bamboo pulp fiber, 20 parts of wood pulp fiber, 20 parts of acrylic fiber, 4 parts of sodium carboxymethyl cellulose 5 parts, 5 parts of nano bamboo charcoal fiber, 10 parts of inorganic filler. The production steps are as follows: 1) Mix bamboo pulp fiber and wood pulp fiber, add water with a mass of 100 times, beat with a beater, control the degree of beating at 40-60° SR, and mix the bamboo pulp fiber and wood pulp fiber 1-2 hours after the start of beating Nano-bamboo charcoal fibers are evenly added to the mixed pulp, and the beating is continued to obtain a mixed pulp of bamboo pulp fibers and wood pulp fibers; 2) Add 100 times of water to the acrylic fibers and beat for 20 to 40 minutes to obtain acrylic fibers 3) mixing bamboo pulp fiber, wood pulp fiber mixed pulp and acrylic fiber pulp in the above st...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com