High-accuracy pressure gauge for measuring pressure
A pressure gauge, high-precision technology, applied in coatings, anti-corrosion coatings, epoxy resin coatings, etc., can solve the problems of small promotion and application prospects, low heat and wear resistance, high production costs, etc., and achieve beautiful appearance and friction resistance Improved capacity and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A high-precision pressure gauge for measuring pressure provided in this embodiment, the surface of the pressure gauge is coated with anti-friction paint, and the composition of the anti-friction paint is calculated in parts by weight: modified alkyd resin: 30 parts, epoxy resin : 20 parts, water-based acrylic resin: 24 parts, ethyl methacrylate: 8 parts, iron powder: 5 parts, deionized water: 20 parts, tung oil: 5 parts, benzophenone: 10 parts, butyl acetate: 15 parts, rosin: 3 parts, matte acrylic paint: 10 parts, aluminum powder: 12 parts, silicon dioxide: 5 parts, polyvinyl butyral: 1 part, additives: 15 parts;
[0024] The components of the auxiliary agent are calculated in parts by weight: kaolin: 22 parts, silane coupling agent: 10 parts, polyvinyl alcohol: 11 parts, talcum powder: 16 parts, paraffin wax: 5 parts, ceramic powder: 3 parts;
[0025] The preparation method of the auxiliary agent is as follows: kaolin and paraffin are mixed and pulverized, passed thro...
Embodiment 2
[0031] A high-precision pressure gauge for measuring pressure provided in this embodiment, the surface of the pressure gauge is coated with anti-friction paint, and the composition of the anti-friction paint is calculated in parts by weight: modified alkyd resin: 32 parts, epoxy resin : 25 parts, water-based acrylic resin: 26 parts, ethyl methacrylate: 10 parts, iron powder: 8 parts, deionized water: 22 parts, tung oil: 8 parts, benzophenone: 12 parts, butyl acetate: 17 parts, rosin: 5 parts, matt acrylic paint: 15 parts, aluminum powder: 14 parts, silicon dioxide: 10 parts, polyvinyl butyral: 3 parts, additives: 20 parts;
[0032] The components of the auxiliary agent are calculated in parts by weight: kaolin: 24 parts, silane coupling agent: 12 parts, polyvinyl alcohol: 13 parts, talcum powder: 18 parts, paraffin wax: 7 parts, ceramic powder: 5 parts;
[0033] The preparation method of the auxiliary agent is as follows: kaolin and paraffin are mixed and pulverized, passed thro...
Embodiment 3
[0039] A high-precision pressure gauge for measuring pressure provided in this embodiment, the surface of the pressure gauge is coated with anti-friction paint, and the composition of the anti-friction paint is calculated in parts by weight: modified alkyd resin: 31 parts, epoxy resin : 24 parts, water-based acrylic resin: 25 parts, ethyl methacrylate: 9 parts, iron powder: 7 parts, deionized water: 21 parts, tung oil: 6 parts, benzophenone: 11 parts, butyl acetate: 16 parts, rosin: 4 parts, matt acrylic paint: 12 parts, aluminum powder: 13 parts, silicon dioxide: 7 parts, polyvinyl butyral: 2 parts, additives: 18 parts;
[0040] The components of the auxiliary agent are calculated in parts by weight: kaolin: 23 parts, silane coupling agent: 11 parts, polyvinyl alcohol: 12 parts, talcum powder: 17 parts, paraffin wax: 6 parts, ceramic powder: 4 parts;
[0041] The preparation method of the auxiliary agent is as follows: kaolin and paraffin are mixed and pulverized, passed thro...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com