A refinery exhaust gas and water washing technology, which is applied in water/sewage treatment, adsorption water/sewage treatment, water/sludge/sewage treatment, etc., can solve the problems of different exhaust gas components, increased treatment costs, and failure to meet discharge standards, etc. , to achieve the effect of convenient use, reducing the difficulty of post-processing, and reducing the cost of post-processing
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] (1) Add 5 parts of silica gel powder and 4 parts of polyacrylamide to 120 parts of n-butanol, heat to reflux state for 10 minutes, then add 5 parts of calcium stearate and 2 parts of sodium silicate, and continue reflux for 5 minutes , to obtain material I;
[0015] (2) Add 10 parts of sodium carboxymethyl cellulose and 8 parts of polyoxyethylene lauryl ether to 800 parts of water, stir to form a uniform solution, then add 4 parts of glucoside and 1 part of urea, mix well and place at 0-5°C Stand still for 8h to obtain material II;
[0016] (3) Add material I, 15 parts of fumed white carbon black, 12 parts of nano-montmorillonite powder, 10 parts of polyaluminum chloride, 6 parts of molecular sieve former powder and 8 parts of ferric sulfate in material II, add in the ball mill after mixing evenly, Ball milling to a fineness of less than 50 μm.
Embodiment 2
[0018] (1) Add 8 parts of silica gel powder and 5 parts of polyacrylamide to 150 parts of n-butanol, heat to reflux state and heat preservation treatment for 10 minutes, then add 3 parts of calcium stearate and 3 parts of sodium silicate, and continue reflux heat preservation treatment for 5 minutes , to obtain material I;
[0019] (2) Add 12 parts of sodium carboxymethyl cellulose and 6 parts of polyoxyethylene lauryl ether to 1000 parts of water, stir to form a uniform solution, then add 6 parts of glucoside and 2 parts of urea, mix well and put it at 0-5°C Stand still for 8h to obtain material II;
[0020] (3) Add material I, 20 parts of fumed white carbon black, 10 parts of nano-montmorillonite powder, 15 parts of polyaluminum chloride, 8 parts of molecular sieve former powder and 5 parts of ferric sulfate in material II, add in the ball mill after mixing evenly, Ball milling to a fineness of less than 50 μm.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com