A cleaning agent and storage tank technology, applied in the field of residual oil storage tank cleaning agents, can solve the problems of contaminated residual oil, corrosion of the inner wall of the storage tank, and easy adhesion on the inner wall of the storage tank, etc., and achieve high cleaning efficiency, convenient use, and excellent The effect of anti-rust effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] (1) Add 6 parts of polyoxyethylene abietic acid and 5 parts of cetyl alcohol to 20 parts of palm oil, first heat to 70-80 °C and mix for 10 minutes, then heat to 100-110 °C and mix for 10 minutes to obtain the material I;
[0016] (2) Add 10 parts of attapulgite and 6 parts of wollastonite powder to 150 parts of ethanol, soak for 30 minutes, and then perform ultrasonic treatment at an ultrasonic frequency of 40 kHz and a power of 100 W for 15 minutes, then add 6 parts of activated alumina and 2 parts of asbestos wool, and continue Ultrasonic treatment for 15 minutes yielded material II;
[0017] (3) Add material I, material II, 10 parts of charcoal powder, 8 parts of polyferric chloride, 6 parts of lauryl polyoxyethylene ether, 3 parts of antirust additives, 2 parts of bamboo vinegar and 2 parts of acetone into 50 parts of acetone Sodium aluminosilicate, mix well.
[0018] Preparation of anti-rust additives: (1) Add 12 parts of tea leaves to 50 parts of water and soak...
Embodiment 2
[0020] (1) Add 8 parts of polyoxyethylene abietic acid ester and 6 parts of cetyl alcohol to 25 parts of palm oil, first heat to 70-80°C and mix for 10 minutes, then heat to 100-110°C for 10 minutes to get the material I;
[0021] (2) Add 15 parts of attapulgite and 4 parts of wollastonite powder to 200 parts of ethanol, after soaking for 30 minutes, ultrasonically treat for 15 minutes at an ultrasonic frequency of 40 kHz and a power of 100 W, then add 8 parts of activated alumina and 3 parts of asbestos wool, continue Ultrasonic treatment for 15 minutes yielded material II;
[0022] (3) Add material I, material II, 15 parts of charcoal powder, 10 parts of polyferric chloride, 4 parts of lauryl polyoxyethylene ether, 4 parts of antirust additives, 3 parts of bamboo vinegar and 1 part of 40 parts of acetone Sodium aluminosilicate, mix well.
[0023] Preparation of anti-rust additives: (1) Add 16 parts of oil tea leaves to 60 parts of water and soak for 12 hours, then add 8 pa...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com