A polyether demulsifier and demulsifier technology, applied in immiscible liquid separation, liquid separation, chemical instruments and methods, etc., can solve the problem of poor broad-spectrum adaptability, unsatisfactory demulsification effect, and unsatisfactory demulsification effect. and other problems, to achieve the effect of fast dehydration rate, ideal dehydration effect and less dosage
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A compound demulsifier for improving the demulsification effect of polyether demulsifiers is obtained by the following method:
[0014] 1) Add 30 grams of polyethylene polyamine and 6 grams of potassium hydroxide into the reactor with a stirring and condensing device, heat up, feed 240 grams of propylene oxide, and control the temperature at 115~145 o C. Under the pressure of 0.4MPa, make it fully react, vacuum for 30 minutes, feed 320 grams of ethylene oxide under the same conditions, after fully reacting, make 600 grams of polyether demulsification.
[0015] 2) Dissolve 600 grams of the above-mentioned polyether demulsifier and 80 grams of high-efficiency flocculant polyacrylamide in 320 grams of methanol, and then stir evenly to obtain a compound demulsifier.
Embodiment 2
[0017] A compound demulsifier for improving the demulsification effect of polyether demulsifiers is obtained by the following method:
[0018] 1) Add 20 grams of pentaerythritol and 4 grams of potassium hydroxide into the reactor with a stirring and condensing device, heat up, feed 160 grams of propylene oxide, and control the temperature at 115~145 o C. Under the pressure of 0.4MPa, make it fully react, vacuum for 30 minutes, feed 210 grams of ethylene oxide under the same conditions, after fully reacting, make 400 grams of polyether demulsification.
[0019] 2) Dissolve 400 grams of the above-mentioned polyether demulsifier and 45 grams of high-efficiency flocculant polyacrylamide in 300 grams of methanol, and then stir evenly to obtain a compound demulsifier.
Embodiment 3
[0021] A compound demulsifier for improving the demulsification effect of polyether demulsifiers is obtained by the following method:
[0022] 1) Add 35 grams of phenolamine resin and 6 grams of potassium hydroxide into the reactor with a stirring and condensing device, heat up, feed 280 grams of propylene oxide, and control the temperature at 115~145 o C. Under the pressure of 0.4MPa, make it fully react, vacuum for 30 minutes, feed 350 grams of ethylene oxide under the same conditions, after fully reacting, make 600 grams of polyether demulsification.
[0023] 2) Dissolve 671 grams of the above-mentioned polyether demulsifier and 78 grams of the high-efficiency flocculant polyacrylamide in 480 grams of methanol and stir evenly to obtain a compound demulsifier.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com