A film-coating agent and chitin technology, applied in the field of medicine, can solve the problems that the ointment formulation is not as convenient as the film-coating agent, the epithelial tissue accelerates the skinning, and the film-forming speed is slow, so as to inhibit the formation of scars, promote growth, and inhibit scar formation. overgrowth effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0028] 1, in the embodiment of the present invention, the proportioning of a kind of chitin anti-scar gel coating agent is:
[0029] Hydroxypropyl Chitosan 2.0g
[0030] Polyvinyl alcohol 4.5g
[0031] Glycerin 2.5g
[0032] Ethanol 8.5g
[0033] Purified water 82.5g
[0034] 2. Preparation method of coating agent
[0035] 1) Prepare 8.5g of ethanol into 20.0% ethanol aqueous solution;
[0036] 2) Dissolve 2.0g hydroxypropyl chitosan in 20.0% ethanol aqueous solution;
[0037] 3) Dissolve 4.5g of polyvinyl alcohol in 40.0g of purified water under heating at 80°C-90°C;
[0038] 4) Mix step 1) with step 2), and add 2.5g glycerin, mix well;
[0039] 5) Vacuumize and fill.
[0040] 3. Performance of coating agent
[0041] 1) Film forming test
[0042] Apply the chitin anti-scar gel coating agent on the dry skin with a thickness of about 1mm. When the room temperature is in the range of 20°C-30°C, it will dry naturally for 3 minutes to 5 minutes to form a transparent film...
Embodiment 2
[0049] 1, in the embodiment of the present invention, the proportioning of a kind of chitin anti-scar gel coating agent is:
[0050] Chitosan quaternary ammonium salt 2.5g
[0051] Polyvinyl alcohol 5.0g
[0052] Propylene glycol 2.0g
[0053] Ethanol 15.0g
[0054] Purified water 75.5g
[0055] 2. Preparation method of coating agent
[0056] 1) Prepare 15.0g of ethanol into 40.0% ethanol aqueous solution;
[0057] 2) 2.5g chitosan quaternary ammonium salt was dissolved in 40.0% ethanol aqueous solution;
[0058] 3) Dissolve 5.0g of polyvinyl alcohol in 38.0g of purified water under heating at 80°C-90°C;
[0059] 4) Mix step 1) with step 2), and add 2.0g propylene glycol, mix well;
[0060] 5) Vacuumize and fill.
[0061] 3. Performance of coating agent
[0062] 1) Film forming test
[0063] Apply the chitin anti-scar gel coating agent on the dry skin with a thickness of about 1mm. When the room temperature is in the range of 20°C-30°C, it will dry naturally for 2.5m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com