Manufacturing method for composite electrolytic plate
A technology of electrolytic plate and preparation steps, applied in electrolytic paint, coating, metal material coating process and other directions, can solve the problems of poor coating adhesion, insufficient hardness of electrolytic plate, poor corrosion resistance and stamping performance, etc. The effect of strong coating adhesion, excellent deep drawing performance and excellent corrosion resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
example 1
[0020] First, soak the cold-rolled steel sheet in acetone solution and let it stand for 10 minutes, then take out the cold-rolled sheet steel, wipe the surface clean, then soak it in the mixed solution, heat it to 55°C, keep it warm for 1 hour, cool it naturally to room temperature, take it out Surface treatment of cold-rolled steel sheets, using distilled water to wash the surface of the surface-treated cold-rolled steel sheets to neutrality, the mixed solution is formed by mixing sodium pyrophosphate, sodium chloride and water in a mass ratio of 1:1:3; then In parts by weight, take 20 parts of disalicylate, 34 parts of distilled water, 6 parts of ammonium bifluoride, 1 part of dodecyl mercaptan and 19 parts of absolute ethanol, and stir evenly to obtain an impregnating solution. The cold-rolled thin steel plate is soaked in the impregnating solution at a solid-to-liquid ratio of 1:4. After standing at room temperature for 1 minute, take out the surface-treated cold-rolled thi...
example 2
[0023] First, soak the cold-rolled steel sheet in the acetone solution and let it stand for 13 minutes, then take out the cold-rolled steel sheet, wipe the surface clean, then soak it in the mixed solution, heat it to 58°C, keep it warm for 1.5h, and cool it down to room temperature naturally. Take out the surface-treated cold-rolled steel sheet, wash the surface of the surface-treated cold-rolled steel sheet with distilled water to neutrality, and the mixed solution is formed by mixing sodium pyrophosphate, sodium chloride and water in a mass ratio of 1:1:3; Then, in parts by weight, take 23 parts of disalicylate, 36 parts of distilled water, 8 parts of ammonium bifluoride, 1.5 parts of dodecyl mercaptan and 20 parts of absolute ethanol, and stir evenly to obtain an impregnation solution. Treat the cold-rolled thin steel plate with a solid-to-liquid ratio of 1:4, soak it in the impregnating solution, let it stand at room temperature for 2 minutes, take out the surface-treated ...
example 3
[0026]First, soak the cold-rolled steel sheet in acetone solution and let it stand for 15 minutes, then take out the cold-rolled sheet steel, wipe the surface clean, then soak it in the mixed solution, heat it to 60°C, keep it warm for 2 hours, cool it naturally to room temperature, take it out Surface treatment of cold-rolled steel sheets, using distilled water to wash the surface of the surface-treated cold-rolled steel sheets to neutrality, the mixed solution is formed by mixing sodium pyrophosphate, sodium chloride and water in a mass ratio of 1:1:3; then In parts by weight, take 25 parts of disalicylate, 38 parts of distilled water, 9 parts of ammonium bifluoride, 2 parts of dodecyl mercaptan and 21 parts of absolute ethanol, and stir evenly to obtain an impregnating solution. The cold-rolled thin steel plate is soaked in the impregnating solution according to the solid-liquid ratio of 1:4, and after standing at room temperature for 3 minutes, the surface-treated cold-roll...
PUM
Property | Measurement | Unit |
---|---|---|
Adhesion amount | aaaaa | aaaaa |
hardness | aaaaa | aaaaa |
hardness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com