Electrode with short production cycle and preparation method thereof
A production cycle and electrode technology, applied in the field of electrodes, can solve the problems of unfavorable promotion and popularization, high cost of small enterprises, time-consuming and laborious costs, etc., and achieve the effects of enhancing electrical conductivity, reducing manufacturing costs, and shortening production cycles.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031] An electrode with a short production cycle, the composition of the electrode with a short production cycle is as follows: 20 parts of needle coke, 8 parts of coal tar pitch, 3 parts of tungsten steel sheets, 3 parts of phenolic resin, and 2 parts of dimethyl phthalate , 10 parts of wire, 4 parts of PVC plastic pipe, 6 parts of silver iodide.
[0032] The present invention also provides a method for preparing an electrode with a short production cycle, comprising the following steps:
[0033] S1. Calcining the needle coke in a calcination furnace at 100°C, then adding coal tar pitch, kneading and pressing to make graphitization;
[0034] S2. After the graphite is formed, take it out and put it in a cooling room with a temperature of -10°C to cool for 15 minutes. The cooling mode of the cooling room is cold air circulation cooling in a closed state;
[0035] S3. While cooling the graphite, polish the tungsten steel sheet smooth with a frosted sheet, and remove the oil st...
Embodiment 2
[0046] An electrode with a short production cycle, the composition of the electrode with a short production cycle is as follows: 25 parts of needle coke, 10 parts of coal tar pitch, 4 parts of tungsten steel sheet, 5 parts of epoxy resin, 4 parts of dimethyl phthalate 13 parts of wire, 5 parts of PVC plastic pipe, and 8 parts of silver iodide.
[0047] The present invention also provides a method for preparing an electrode with a short production cycle, comprising the following steps:
[0048] S1. Calcining the needle coke in a calcination furnace at 130°C, and then adding coal tar pitch to make graphitization through kneading and pressing;
[0049] S2. After the graphite is formed, take it out and put it in a cooling room with a temperature of -15°C to cool for 20 minutes. The cooling mode of the cooling room is cold air circulation cooling in a closed state;
[0050] S3. While cooling the graphite, polish the tungsten steel sheet smooth with a frosted sheet, and remove the oi...
Embodiment 3
[0061] An electrode with a short production cycle, the composition of the electrode with a short production cycle is as follows: 30 parts of petroleum coke, 12 parts of coal tar pitch, 5 parts of tungsten steel sheet, 8 parts of furfuryl alcohol resin, 6 parts of dimethyl phthalate, 15 parts of wire, 6 parts of PVC plastic pipe, 10 parts of silver iodide.
[0062] The present invention also provides a method for preparing an electrode with a short production cycle, comprising the following steps:
[0063] S1. Calcining petroleum coke in a calcination furnace at 150°C, and then adding coal tar pitch to make graphitization through kneading and pressing;
[0064] S2. After the graphite is formed, take it out and put it in a cooling room at -20°C for 15-25 minutes. The cooling mode of the cooling room is cold air circulation cooling in a closed state;
[0065] S3. While cooling the graphite, polish the tungsten steel sheet smooth with a frosted sheet, and remove the oil stains an...
PUM