[0016] A kind of willow paint made of wicker, made of the following components by weight: silicon acrylic emulsion 80, modifier 1, composite filler 25, sodium dodecylbenzene sulfonate 1, ammonium polyphosphate 10, polyurethane emulsion 2, Borate 3, modified tree sap 5, dioctyl phthalate 1, trisodium phosphate 2, turpentine oil and lignin blend 4, water 48.
[0017] Further, the composite filler is made of the following components in parts by weight: nano-alumina 5, calcium carbonate 6, and perlite 1.
[0018] Further, the preparation method of the modified mulberry sap is as follows: seal and heat the mulberry sap to 68°C, keep it warm for 10 minutes, add 0.5% sodium hydroxide of the mulberry sap mass, and stir at 120r / min for 20 minutes Finally, add dibutyltin dilaurate with a mass of 0.01% of mulberry sap, raise the temperature to 75°C, stir at a speed of 150r / min for 15 minutes, keep it warm for 20 minutes, then cool to 12°C, and keep it warm for 15 minutes After that, ret...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com