Antibacterial peptide finishing process for wool fabric
An antibacterial peptide and wool technology, applied in fiber treatment, animal fiber, biochemical fiber treatment, etc., can solve the problem of lack of antibacterial wool fabrics, and achieve the effects of excellent antibacterial properties, small relative molecular weight, and improved washability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0016] For realizing above-mentioned technical effect, the antimicrobial peptide finishing process of woolen fabric in embodiment 1, comprises the following steps:
[0017] S1: Wool fabric oxidation pretreatment, the wool fabric is put into the oxidation treatment solution for 35 minutes, then washed with distilled water and dried, the oxidation treatment solution contains hydrogen peroxide, sodium silicate and penetrant, the concentration of hydrogen peroxide is 30ml / L, oxidation treatment The pH of the solution is 8;
[0018] S2: antimicrobial peptide buffer solution treatment, the woolen fabric obtained in S1 is treated with antimicrobial peptide buffer solution padding method, and the ratio of the consumption of antimicrobial peptide to the wool fabric weight is 0.7ml / g;
[0019] S3: Curing and crosslinking treatment, the wool fabric obtained in S2 is treated with a glutaraldehyde mixed solution padding method, placed in a constant temperature shaker at a constant temperat...
Embodiment 2
[0025] The antimicrobial peptide finishing process of wool fabric in embodiment 2 may further comprise the steps:
[0026] S1: Wool fabric oxidation pretreatment, the wool fabric is put into the oxidation treatment solution for 50 minutes, then washed with distilled water, and dried. The oxidation treatment solution contains hydrogen peroxide, sodium silicate and penetrating agent. The concentration of hydrogen peroxide is 45ml / L. The pH value of the solution is 8.25;
[0027] S2: antimicrobial peptide buffer solution treatment, the wool fabric obtained in S1 is treated with antimicrobial peptide buffer solution padding method, and the ratio of the consumption of antimicrobial peptide to the weight of wool fabric is 1.1ml / g;
[0028] S3: Curing and cross-linking treatment, the wool fabric obtained in S2 is treated with a glutaraldehyde mixed solution padding method, placed in a constant temperature shaker at a constant temperature of 27 ° C for 5 hours, washed with distilled w...
Embodiment 3
[0034] The antimicrobial peptide finishing process of wool fabric in embodiment 3 may further comprise the steps:
[0035] S1: Wool fabric oxidation pretreatment, the wool fabric is put into the oxidation treatment solution for 80 minutes, then washed with distilled water and dried, the oxidation treatment solution contains hydrogen peroxide, sodium silicate and penetrant, the concentration of hydrogen peroxide is 60ml / L, oxidation treatment The pH of the solution is 8.5;
[0036] S2: antimicrobial peptide buffer solution treatment, the wool fabric obtained in S1 is treated with antimicrobial peptide buffer solution padding method, and the ratio of the consumption of antimicrobial peptide to the weight of wool fabric is 1.5ml / g;
[0037] S3: Curing and cross-linking treatment, the wool fabric obtained in S2 is treated by padding method with glutaraldehyde mixed solution, placed in a constant temperature shaker at a constant temperature of 25-30 ° C for 6 hours, washed with dis...
PUM