Sodium percarbonate cashmere bleaching solution and bleaching method thereof
A sodium percarbonate and bleaching solution technology, applied in textiles and papermaking, can solve the problems of cashmere fiber strength loss, improper control of bleaching process parameters, affecting spinning yield and finished product handle, etc., and achieve good water solubility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] For realizing above-mentioned technical effect, sodium percarbonate cashmere bleaching liquid component comprises sodium percarbonate 0.3%, bleaching activator 0.05%, composite oxygen bleaching stabilizer, pH value regulator and water by weight percentage in embodiment 1, percarbonate Sodium cashmere bleach has a pH of 8.5.
[0018] Wherein, the pH regulator is sodium hydroxide.
[0019] Among them, the composition of the composite oxygen bleaching stabilizer is: 8 parts of tartaric acid, 2 parts of polymalic acid, 10 parts of talcum powder, 20 parts of ethanol, 3 parts of hydroxyethylene diphosphoric acid, and 60 parts of water.
[0020] Wherein, the bleach activator is nonanoyloxybenzenesulfonate.
[0021] The bleaching method of sodium percarbonate cashmere bleaching solution may further comprise the steps:
[0022] S1: Put the cashmere fiber into the sodium percarbonate cashmere bleaching solution to fully soak at room temperature, gradually raise the temperature ...
Embodiment 2
[0027] In embodiment 2, sodium percarbonate cashmere bleach component comprises sodium percarbonate 0.7%, bleach activator 0.15%, composite oxygen bleach stabilizer, pH regulator and water by weight percentage, the pH of sodium percarbonate cashmere bleach The value is 9.
[0028] Wherein, the pH regulator is glycine-sodium hydroxide pH buffer pair.
[0029] Among them, the composition of the composite oxygen bleaching stabilizer is: 9 parts of tartaric acid, 3.5 parts of polymalic acid, 15 parts of talcum powder, 30 parts of ethanol, 4.5 parts of hydroxyethylene diphosphoric acid, and 50 parts of water.
[0030] Wherein, the bleach activator is formed by mixing tetraacetylethylenediamine and hexamethylenetetramine at a ratio of 1:1.
[0031] The bleaching method of sodium percarbonate cashmere bleaching solution may further comprise the steps:
[0032] S1: Put the cashmere fiber into the sodium percarbonate cashmere bleaching solution to fully soak at room temperature, grad...
Embodiment 3
[0037] In embodiment 3, sodium percarbonate cashmere bleaching solution component comprises sodium percarbonate 1.2%, bleach activator 0.25%, composite oxygen bleach stabilizer, pH regulator and water by weight percentage, the pH of sodium percarbonate cashmere bleaching solution The value is 9.5.
[0038] Wherein, the pH regulator is a sodium carbonate-sodium bicarbonate pH buffer pair.
[0039] Among them, the composition of the composite oxygen bleaching stabilizer is: 10 parts of tartaric acid, 2 parts of polymalic acid, 20 parts of talcum powder, 40 parts of ethanol, 6 parts of hydroxyethylene diphosphoric acid, and 40 parts of water.
[0040] Wherein, the bleach activator is at least one selected from tetraacetylethylenediamine, nonanoyloxybenzenesulfonate, diethyl tartrate, amine acetate, and hexamethylenetetramine.
[0041] The bleaching method of sodium percarbonate cashmere bleaching solution may further comprise the steps:
[0042] S1: Put the cashmere fiber into ...