An interior wall latex paint and high-adhesion technology, applied in the field of latex paint, can solve the problems affecting the latex paint adhesion, durability, water resistance, performance can not meet the needs, the human body damage is relatively large, etc., to improve the anti-fouling. ability, improved scrub resistance, soft and bright color effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0022] A high-adhesive interior wall latex paint, according to the weight ratio, the latex paint consists of 60 parts of titanium dioxide, 50 parts of high titanium powder, 100 parts of salt gypsum powder, 40 parts of talcum powder, 40 parts of heavy calcium powder, and 2 parts of photocatalyst , 1 part of ethylene glycol ether acetate, 1 part of defoamer, 2 parts of dispersant, 2 parts of thickener, 0.6 part of antioxidant, 1.5 part of antifungal agent, 120 parts of deionized water, 70 parts of acrylate emulsion and 10 parts of wolfberry extract, said wolfberry extract is the juice obtained from the fresh leaves obtained from wolfberry after squeezing and filtering and sodium dodecylbenzenesulfonate according to the weight ratio of 100:1 Mixed and stirred for 1h to obtain;
[0023] The preparation method of the above-mentioned high-adhesive interior wall latex paint, first prepares the wolfberry extract, then weighs each raw material according to the above requirements, and m...
Embodiment 2
[0032] A high-adhesion latex paint for interior walls. According to the weight ratio, the latex paint consists of 90 parts of titanium dioxide, 70 parts of high-titanium powder, 120 parts of salt gypsum powder, 60 parts of talcum powder, 60 parts of heavy calcium powder, and 4 parts of photocatalyst. , 3 parts of ethylene glycol ether acetate, 3 parts of defoamer, 3 parts of dispersant, 3 parts of thickener, 1 part of antioxidant, 3 parts of antifungal agent, 140 parts of deionized water, 90 parts of acrylate emulsion and 15 parts of wolfberry extracts, said wolfberry extracts obtained from the fresh leaves of wolfberry after squeezing and filtering the juice and sodium dodecylbenzene sulfonate according to the weight ratio of 100:2 Mixed and stirred for 1h to obtain;
[0033] The preparation method of the above-mentioned high-adhesive interior wall latex paint firstly prepares the wolfberry extract, then weighs each raw material according to the above-mentioned requirements, ...
Embodiment 3
[0042]A high-adhesion latex paint for interior walls. According to the weight ratio, the latex paint consists of 80 parts of titanium dioxide, 60 parts of high titanium powder, 110 parts of salt gypsum powder, 50 parts of talcum powder, 50 parts of heavy calcium powder, and 3 parts of photocatalyst , 2 parts of ethylene glycol ether acetate, 2 parts of defoamer, 2.5 parts of dispersant, 2.5 parts of thickener, 0.8 parts of antioxidant, 2 parts of antifungal agent, 130 parts of deionized water, 80 parts of acrylate emulsion and 11 parts of wolfberry extract, which is obtained from the fresh leaves of wolfberry after squeezing and filtering the juice and sodium dodecylbenzenesulfonate according to the weight ratio of 100:1.3 Mixed and stirred for 1h to obtain;
[0043] The preparation method of the above-mentioned high-adhesive interior wall latex paint firstly prepares the wolfberry extract, then weighs each raw material according to the above-mentioned requirements, and mixes ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com