Embodiment 1
[0025] The wood for furniture is carefully selected and sent to the drying room, where it is dried on the kang at a temperature of 70°C and a humidity of 50% for 6 hours, and then used to make furniture. Send the furniture to the sanding machine to sand the outer surface of the furniture. First use 240♯ sandpaper for rough sanding, and then use 320♯ sandpaper for simple polishing to remove stains and smooth. Mix the two-component water-based special sealing primer and water in a ratio of 0.85: 0.15, and use an automatic roller coater to continuously roll coat the outer surface of the furniture twice. The furniture after the primer roll coating is sent to the UV drying tunnel. The temperature in the UV drying tunnel is 100 ℃. After drying at this temperature for 1.2 hours, the drying stops, and the air is sent to the UV drying tunnel through the air supply device Perform cooling to room temperature. Send the furniture to the sanding machine, and use a 600♯ sanding belt to polis...
Embodiment 2
[0027] The wood for furniture is carefully selected and sent to the drying room, where it is dried on the kang at a temperature of 70°C and a humidity of 50% for 6.5 hours, and then used to make furniture. Send the furniture to the sanding machine to sand the outer surface of the furniture. First use 240♯ sandpaper for rough sanding, and then use 320♯ sandpaper for simple polishing to remove stains and smooth. Mix the two-component water-based special sealing primer and water in a ratio of 0.875:0.125, and use an automatic roller coater to continuously roll coat the outer surface of the furniture 3 times. The furniture after the primer roller coating is sent to the ultraviolet light drying tunnel. The temperature in the ultraviolet light drying tunnel is 110℃. After drying at this temperature for 1.1 hours, the drying stops, and air is sent to the ultraviolet light drying tunnel through the air supply device Perform cooling to room temperature. Send the furniture to the sandin...
Embodiment 3
[0029] The wood for furniture is carefully selected and sent to the drying room, where it is dried on the kang at a temperature of 70°C and a humidity of 50% for 7 hours, and then used to make furniture. Send the furniture to the sanding machine to sand the outer surface of the furniture. First use 240♯ sandpaper for rough sanding, and then use 320♯ sandpaper for simple polishing to remove stains and smooth. Mix the two-component water-based special sealing primer and water in a ratio of 0.90:0.10, and use an automatic roller coater to continuously roll coat the outer surface of the furniture 3 times. The furniture after the primer roller coating is sent to the ultraviolet light drying tunnel. The temperature in the ultraviolet light drying tunnel is 120℃. After drying at this temperature for 1 hour, the drying stops, and the air supply device sends air to the ultraviolet light drying tunnel. Perform cooling to room temperature. Send the furniture to the sanding machine, and u...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com