[0018] An environmentally friendly paint is composed of the following raw materials in parts by weight: 52 parts of water, 5 parts of seaweed mud, 10 parts of talcum powder, 20 parts of lime calcium powder, 5 parts of white charcoal, 12 parts of white cement and 3 parts of thickener.
[0019] As a further solution of the present invention: the thickener is composed of the following raw materials in parts by weight: 4 parts of stearic acid, 5 parts of sodium alginate, 3 parts of silicon dioxide, 8 parts of cellulose ether and 5 parts of bentonite.
[0020] A kind of preparation method of environment-friendly paint, its main steps are as follows:
[0021] The first step: weighing raw materials according to parts by weight;
[0022] Step 2: Add seaweed mud, talcum powder, gray calcium powder, white charcoal and white cement into the mixer according to the weight and stir evenly to form a solid mixture;
[0023] The third step: add water to the mixture in the second step, stir ev...
Embodiment 2
[0025] An environmentally friendly paint is composed of the following raw materials in parts by weight: 55 parts of water, 6 parts of seaweed mud, 11 parts of talcum powder, 25 parts of lime calcium powder, 8 parts of white charcoal, 14 parts of white cement and 4 parts of thickener.
[0026] As a further solution of the present invention: the thickener is composed of the following raw materials in parts by weight: 5 parts of stearic acid, 6 parts of sodium alginate, 4 parts of silicon dioxide, 10 parts of cellulose ether and 8 parts of bentonite.
[0027] A kind of preparation method of environment-friendly paint, its main steps are as follows:
[0028] The first step: weighing raw materials according to parts by weight;
[0029] Step 2: Add seaweed mud, talcum powder, gray calcium powder, white charcoal and white cement into the mixer according to the weight and stir evenly to form a solid mixture;
[0030] The third step: add water to the mixture in the second step, stir e...
Embodiment 3
[0032] An environmentally friendly paint is composed of the following raw materials in parts by weight: 60 parts of water, 8 parts of seaweed mud, 12 parts of talcum powder, 24 parts of lime calcium powder, 14 parts of white charcoal, 14 parts of white cement and 4 parts of thickener.
[0033] As a further solution of the present invention: the thickener is composed of the following raw materials in parts by weight: 6 parts of stearic acid, 6 parts of sodium alginate, 4 parts of silicon dioxide, 10 parts of cellulose ether and 9 parts of bentonite.
[0034] A kind of preparation method of environment-friendly paint, its main steps are as follows:
[0035] The first step: weighing raw materials according to parts by weight;
[0036] Step 2: Add seaweed mud, talcum powder, gray calcium powder, white charcoal and white cement into the mixer according to the weight and stir evenly to form a solid mixture;
[0037] The third step: add water to the mixture in the second step, stir ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com