A color depth, cotton fabric technology, applied in dyeing, textile and papermaking, etc., can solve the problems of light color and instability of natural brown cotton fabrics, improve stability, avoid environmental pollution problems, wash fastness and daily life. The effect of improving light fastness
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0031] The natural brown cotton fabric used in this embodiment is a natural brown cotton woven fabric without desizing and scouring treatment, and the chromaticity data of the fabric are: L*=55.61, a*=14.33, b*=30.22, K / S =2.96.
[0032] A method for improving the color depth and fastness of natural brown cotton fabrics, comprising the steps of:
[0033] 1) Preparation of darkening solution: Weigh and mix 0.5Kg of sodium hydroxide, 4.5Kg of sodium carbonate, 1Kg of fatty alcohol polyoxyethylene ether, 1Kg of sodium dodecylbenzenesulfonate and 800Kg of water, and stir evenly to obtain the darkening solution. solution, ready to use;
[0034] 2) Preparation of color-fixing solution: Weigh and mix 3Kg of cerium dioxide, 1Kg of glyceryl monostearate and 800Kg of water, and disperse for 60 minutes under the assistance of ultrasonic waves (power 250W, rated frequency 40KHz) to form a suspension system, namely It is a color-fixing solution, ready for use;
[0035] 3) Pretreatment: ...
Embodiment 2
[0041]The natural brown cotton fabric used in this embodiment is a natural brown cotton woven fabric without desizing and scouring treatment, and the chromaticity data of the fabric are: L*=55.61, a*=14.33, b*=30.22, K / S =2.96.
[0042] A method for improving the color depth and fastness of natural brown cotton fabrics, comprising the steps of:
[0043] 1) Preparation of darkening solution: weigh and mix 1.5Kg of sodium hydroxide, 13.5Kg of sodium carbonate, 3Kg of sodium alkyl sulfate, 3Kg of sodium fatty alcohol polyoxyethylene ether sulfate and 1000Kg of water, and stir evenly to obtain the darkening solution ,stand-by;
[0044] 2) Preparation of color fixing solution: Weigh and mix 5Kg of lanthanum oxide, 3Kg of sorbitan fatty acid and 1000Kg of water, and disperse for 120 minutes with the assistance of ultrasonic waves (500W power, 40KHz rated frequency) to form a suspension system, which is color fixing solution, ready to use;
[0045] 3) Pretreatment: immerse 10Kg of...
Embodiment 3
[0050] The natural brown cotton fabric used in this embodiment is a natural brown cotton knitted fabric without scouring treatment, and the chromaticity data of the fabric are: L*=51.93, a*=14.08, b*=30.10, K / S=3.21.
[0051] A method for improving the color depth and fastness of natural brown cotton fabrics, comprising the steps of:
[0052] 1) Preparation of darkening solution: Weigh and mix 1.5Kg of sodium hydroxide, 12Kg of sodium carbonate, 2Kg of sodium alkyl sulfosuccinate, 2Kg of alkylphenol polyoxyethylene ether and 900Kg of water, and stir evenly to obtain the darkening solution. solution, ready to use;
[0053] 2) Preparation of color fixing solution: Weigh and mix 4Kg of praseodymium and neodymium oxide, 2Kg of 2Kg of polyoxyethylene 2-octylphenol and 900Kg of water, and disperse for 90 minutes under the assistance of ultrasonic waves (power 400W, rated frequency 40KHz) to form a suspension system , which is the color-fixing solution, ready for use;
[0054] 3) P...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com