A technology of polymer materials and condoms, which is applied in the application, household components, household appliances, etc., can solve the problem that the stretch thinness or toughness sensitivity of condoms is not improved, and the sensitivity and skin-friendly texture of condoms without polymer materials are synthesized. problem, to achieve a good effect of sensitivity and skin-friendly texture
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0018] Embodiment 1 A kind of method adopting polymer material mixing to prepare novel condom, comprises the following steps:
[0019] A1: Mix and mix polyvinyl alcohol, silk protein, cyclodextrin, chitosan, montmorillonite, and deionized water at 100°C, then add polyurethane latex for mixing, and control the temperature during the mixing process. The total solid content is 20%, the pH value is 5.5-7.0 to obtain the mixed latex, and the mixed latex is parked and matured;
[0020] A2: Dip a condom mold with a suitable shape into the mixed latex matured in step A1, take out the condom mold after dipping and dry it at 100°C to form a film on the condom mold;
[0021] A3: The film formed on the condom mold described in step A2 is conventionally crimped, dried, swollen, stripped, soaked, powdered, and dehydrated, and then dried at 100°C to form condoms.
[0022] The preferred technical solution of this embodiment is that in step A1, the mixing process is stirred at 100° C. for 30...
Embodiment 2
[0029] Example 2 On the basis of Example 1, a nano-scale graphene oxide chip is implanted during step A2, and after post-processing, the user can visualize the data in sexual life through terminal APPs such as mobile phones, computers, and smart watches ( How many calories are burned by physical energy, twitch frequency, posture, internal vision, temperature, etc.).
[0030] The mixed latex formula that the present invention adopts is as shown in the following table:
[0031] Ingredients function
Solid material ratio (weight parts)
242g 40%
0.54 grams
silk protein
0.54 grams
0.9 grams
0.9 grams
0.6 grams
Deionized water
254.8 grams
0.001g
anti-sticking agent
0.01g
Silica
0.1-0.3 grams
total
Appropriate amount (determined by total solids content)