A production process of lithium-ion battery tabs with high sealing and anti-leakage

A lithium-ion battery and production process technology, applied in electrode manufacturing, electrode forming, secondary batteries, etc., can solve problems such as electrolyte leakage, bonding effect is not as good as the same material, and endanger user safety, so as to improve quality and Safety, ease of soldering handling, and the effect of improving soldering performance

Active Publication Date: 2020-03-17
赣州市中金高能电池材料股份有限公司
View PDF2 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

And if the lithium-ion battery is not well sealed, the electrolyte may leak, which will lead to the failure of the battery cell, that is, the battery is scrapped.
In the complete sealing body of aluminum-plastic film packaging bag, other parts are welded by the same non-metallic material, and the welding effect is like a whole. Only the tabs are bonded between metal and non-metal, and the bonding effect is far less than The same material, therefore, the seal of the tab part is the weakest, and once the sealing and bonding interface fails, it will cause the lithium-ion battery to leak and the entire lithium-ion battery will fail, and even fire and other related safety accidents will occur. endanger the safety of users

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] The production process of the lithium-ion battery tab with high sealing and anti-leakage, the specific steps are:

[0028] A. Carrying out bright rolling molding of the base metal material through a double-roll rolling machine to obtain a bright strip-shaped metal conductor;

[0029] B. Carry out sand blasting treatment to the roll of the rolling mill, and pass the bright strip-shaped metal conductor through the rolling mill of the roll to carry out matte rolling and shaping, obtain the matte strip-shaped metal conductor, make its surface roughness reach 30μm;

[0030] C. Carry out electrochemical polishing to the dull strip-shaped metal conductor to make its surface roughness reach 15 μm, and clean and dry it;

[0031] D. Passivate the matte strip-shaped metal conductor (wherein, if the metal conductor material is aluminum, it can be directly passivated; if the metal conductor material is copper, it needs to be nickel-plated first, and then cleaning and drying, and t...

Embodiment 2

[0038] The production process of the lithium-ion battery tab with high sealing and anti-leakage, the specific steps are:

[0039] A. Carrying out bright rolling molding of the base metal material through a double-roll rolling machine to obtain a bright strip-shaped metal conductor;

[0040]B. Electroetching is carried out to the roll of the rolling mill, and the bright strip-shaped metal conductor is passed through the rolling mill of the roll for matte rolling and shaping, so as to obtain a matt strip-shaped metal conductor, and its surface roughness reaches 35μm;

[0041] C. Carry out electrochemical polishing to the dull strip-shaped metal conductor again to make its surface roughness reach 17 μm, and clean and dry it;

[0042] D. Passivate the matte strip-shaped metal conductor (wherein, if the metal conductor material is aluminum, it can be directly passivated; if the metal conductor material is copper, it needs to be nickel-plated first, and then cleaning and drying, a...

Embodiment 3

[0049] The production process of the lithium-ion battery tab with high sealing and anti-leakage, the specific steps are:

[0050] A. Carrying out bright rolling molding of the base metal material through a double-roll rolling machine to obtain a bright strip-shaped metal conductor;

[0051] B. Carry out laser etching sand treatment on the roll of the rolling mill, and pass the bright strip-shaped metal conductor through the rolling mill of the roll for matte rolling and shaping to obtain a matt strip-shaped metal conductor to make the surface roughness up to 40μm;

[0052] C. Carry out electrochemical polishing to the dull strip-shaped metal conductor to make its surface roughness reach 20 μm, and clean and dry it;

[0053] D. Passivate the matte strip-shaped metal conductor (wherein, if the metal conductor material is aluminum, it can be directly passivated; if the metal conductor material is copper, it needs to be nickel-plated first, and then cleaning and drying, and then...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
surface roughnessaaaaaaaaaa
surface roughnessaaaaaaaaaa
surface roughnessaaaaaaaaaa
Login to view more

Abstract

The invention discloses a production process of lithium-ion battery tabs with high sealing and anti-leakage. In the production process, the base metal material is subjected to bright rolling and dull rolling through steps A-H, and then electrochemically polished and polished. passivation, cleaning and drying it, and then cut the strip-shaped metal conductor into sections, ultrasonic cleaning and drying it, and treating it with deionized water and drying it, and finally strip The polymer insulating film is pasted on the segmented metal conductor. The lithium-ion battery tab produced by this process increases the surface roughness of the metal conductor, which increases the effective contact area between the metal conductor and the polymer insulating film, so it can effectively improve the adhesion and make the two bonds more stable, thereby Improve the sealing performance of the battery cell and improve the welding performance of the metal conductor. At the same time, it reduces the surface activity of the metal conductor and enhances its ability to resist electrolyte erosion, thereby further improving the sealing performance of the battery cell and preventing lithium-ion batteries from leaking.

Description

technical field [0001] The invention relates to a production process of a lithium ion battery tab, in particular to a production process of a lithium ion battery tab with high sealing and anti-leakage. Background technique [0002] Lithium-based batteries can be divided into lithium batteries and lithium-ion batteries. Among them, lithium-ion batteries are a kind of secondary batteries (rechargeable batteries), which mainly rely on lithium ions to move between the positive and negative electrodes to work; during charging and discharging, Li + intercalation and deintercalation back and forth between the two electrodes; when charging, the Li + It is deintercalated from the positive electrode, inserted into the negative electrode through the electrolyte, and the negative electrode is in a lithium-rich state; the opposite is true during discharge. Nowadays, electrical components such as mobile phones and laptops use lithium-ion batteries, commonly known as lithium batteries. B...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): H01M4/04H01M10/0525H01M2/26H01M50/531
CPCH01M4/0433H01M10/0525H01M50/531Y02E60/10
Inventor 邓国梁李宇明胡昌军周燕飞南春雷
Owner 赣州市中金高能电池材料股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products