Printing adhesive capable of achieving cloth surface soft handfeel and high tearing strength, and preparation method thereof
A tear strength and adhesive technology, which is applied in dyeing, textiles and papermaking, etc., can solve the problems of lower production efficiency, solvent resistance, cumbersomeness, etc., and achieve the effects of reducing costs, simple methods, and improving efficiency
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] A printing adhesive with soft handfeel and high tear strength on cloth and a preparation method thereof, comprising the following percentages: 300 parts of butyl acrylate, 30 parts of isobornyl methacrylate, 20 parts of isooctyl acrylate, and methylenebispropylene 0.2 parts of amide, 6 parts of acrylic acid, 4 parts of itaconic acid, 2.5 parts of diacetone acrylamide or silane coupling agent 151, 1.5 parts of acrylamide, 15 parts of Pingpingjia, 10 parts of A-980 (Shanghai Zhongyi Chemical Emulsifier) , 10 parts of Ks-360 (Shanghai Zhongyi Chemical Emulsifier), 1 part of ammonia water, 600 parts of deionized water, put the monomer components into the emulsification tank, add the deionized water dispersion and stir at 2800r / min for 1h, emulsify The solution was put into a 1000ml plastic bottle and irradiated by a radiation source for 4h.
[0021] The preparation method is as follows:
[0022] Step 1: monomer components, 300 parts of butyl acrylate, 30 parts of isobornyl...
Embodiment 2
[0029] A printing adhesive with soft handfeel and high tear strength on cloth and a preparation method thereof, comprising the following percentages: 300 parts of butyl acrylate, 30 parts of isobornyl methacrylate, 20 parts of isooctyl acrylate, and methylenebispropylene 0.6 parts of amide, 6 parts of acrylic acid, 4 parts of itaconic acid, 2.8 parts of diacetone acrylamide or silane coupling agent 151, 1.8 parts of acrylamide, 15 parts of Pingpingjia, 10 parts of A-980 (Shanghai Zhongyi Chemical Emulsifier) , 10 parts of Ks-360 (Shanghai Zhongyi Chemical Emulsifier), 1 part of ammonia water, 600 parts of deionized water, put the monomer components into the emulsification tank, add the deionized water dispersion and stir at 2800r / min for 1h, emulsify The solution was put into a 1000ml plastic bottle and irradiated by a radiation source for 5 hours.
[0030] The preparation method is as follows:
[0031] Step 1: monomer components, 300 parts of butyl acrylate, 30 parts of isob...
Embodiment 3
[0038] A printing adhesive with soft handfeel and high tear strength on cloth and a preparation method thereof, comprising the following percentages: 300 parts of butyl acrylate, 30 parts of isobornyl methacrylate, 20 parts of isooctyl acrylate, and methylenebispropylene 1 part of amide, 6 parts of acrylic acid, 4 parts of itaconic acid, 3 parts of diacetone acrylamide or silane coupling agent 151, 2 parts of acrylamide, 15 parts of Pingpingjia, 10 parts of A-980 (Shanghai Zhongyi Chemical Emulsifier) , 10 parts of Ks-360 (Shanghai Zhongyi Chemical Emulsifier), 1 part of ammonia water, 600 parts of deionized water, put the monomer components into the emulsification tank, add the deionized water dispersion and stir at 2800r / min for 1h, emulsify The solution was put into a 1000ml plastic bottle and irradiated by a radiation source for 6 hours.
[0039] The preparation method is as follows:
[0040] Step 1: monomer components, 300 parts of butyl acrylate, 30 parts of isobornyl m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com