A loaded activated carbon with indoor formaldehyde removal and bactericidal and anti-mildew functions
A technology of activated carbon and formaldehyde, applied in the directions of fungicides, botanical equipment and methods, biocides, etc., can solve the problems of easy breeding of bacteria and molds, low processing rate, peculiar smell, etc. stable effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0056] The present invention also provides a kind of preparation method of above-mentioned supported activated carbon, and this method comprises the following steps:
[0057] (1) The activated carbon carrier is loaded with a water-soluble inorganic base and a bactericide to obtain activated carbon loaded with a bactericide.
[0058] Preferably, the water-soluble inorganic base and the fungicide are dissolved in water, the activated carbon carrier is added, after impregnated, dried to obtain the activated carbon loaded with the fungicide.
[0059] Wherein, the mass ratio of water-soluble inorganic base to water is 1-10%, preferably 2-8%, most preferably 3-7%; the mass ratio of fungicide to water is 5-20%, preferably 5-16% %, most preferably 8-13%; the water-soluble inorganic base and bactericide in the mass ratio can make the activated carbon carrier load a sufficient load.
[0060] When the load of the fungicide on the activated carbon is low, it will affect the killing effec...
Embodiment 1
[0079] Prepare 200 g of a mixed solution of sodium hydroxide and polyhexamethylene biguanide hydrochloride, wherein the mass ratio of sodium hydroxide is 5%, and the mass ratio of polyhexamethylene biguanide hydrochloride is 10.5%.
[0080] Weigh 100 grams of raw carbon with a carbon tetrachloride adsorption rate of 100%, immerse the raw carbon in the mixed solution for 1 hour, take it out after the immersion is completed, and dry it at 130 ° C for 3 hours to obtain 120.5 grams of product.
[0081] Through testing, the product is loaded with 4.1% sodium hydroxide, 10.1% loaded polyhexamethylene biguanide hydrochloride, and 6.3% water content.
Embodiment 2
[0083] Prepare 200 g of a mixed solution of sodium hydroxide and polyhexamethylene biguanide hydrochloride, wherein the mass ratio of sodium hydroxide is 7%, and the mass ratio of polyhexamethylene biguanide hydrochloride is 12%.
[0084] Weigh 150 grams of raw carbon with a carbon tetrachloride adsorption rate of 70%, soak the raw carbon in the mixed solution for 2 hours, take it out after the immersion is completed, and dry it at 150° C. for 3 hours to obtain 173 grams of product.
[0085] Through testing, the product is loaded with 5.9% sodium hydroxide, 12.9% loaded polyhexamethylene biguanide hydrochloride, and 4.7% water content.
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com