Preparation method of stainless steel wire modified by Bi2WO6 glass ceramics for dynamic intercepting
A technology of glass-ceramic and stainless steel wire, which is applied in the preparation of Bi2WO6 glass-ceramic modification and the preparation of Bi2WO6 glass-ceramic modification with stainless steel wire for dynamic interception, which can solve the problem of PM2.5 index increase, low purification rate and oil fume interception rate Problems such as not achieving the desired effect, to achieve the effect of simple process
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0023] The dynamic interception provided by the present embodiment uses the stainless steel wire Bi 2 WO 6 A method for preparing glass-ceramics modification, comprising the steps of:
[0024] Step 1: Preparation of Bi 2 WO 6 Micro-powder of glass-ceramic for preparing Bi 2 WO 6 The particle size of glass-ceramic powder is 0.1-10um, Bi 2 WO 6 The concrete component of glass-ceramic micropowder can be Bi 2 WO 6 Glass-ceramic, also B 2 o 3 Bi 2 o 3 WO 3 or graphene hybrid Li 2 B 4 o 7 Bi 2 WO 6 One of them and their modified components, the modified components can be Bi 2 WO 6 / BiVO 4 / carbon nanotube or Bi 2 WO 6 / BiVO 4 / coconut carbon;
[0025] Step 2: Treat the surface of the stainless steel wire for dynamic interception by thermal spraying, and apply Bi 2 WO 6 Glass-ceramic powder is thermally sprayed onto the surface of stainless steel wire for dynamic interception to make Bi 2 WO 6 Stainless steel wire is used for dynamic interception of glass...
Embodiment 1
[0029] The dynamic interception that present embodiment 1 provides is used stainless steel wire Bi 2 WO 6 The preparation method of glass-ceramics modification comprises the steps of: preparing graphene hybrid Bi 2 WO 6 Glass-ceramic powder to 1um size, using a plasma spraying device to prepare graphene-containing hybrid Bi 2 WO 6 Glass-ceramic powder coating the surface of stainless steel wire for dynamic interception, mixing graphene with Bi 2 WO 6 The stainless steel wire used for dynamic interception of glass-ceramic glaze is placed in the dynamic interception device to realize Bi 2 WO 6 The self-cleaning and VOC degradation functions of the stainless steel wire used for the dynamic interception of the glass-ceramic glaze, this embodiment 1 makes full use of the heat energy and light energy of the cooktop itself, energy saving and environmental protection, one thing with multiple functions, and the process is simple.
Embodiment 2
[0031] The dynamic intercepting stainless steel wire Bi that present embodiment 2 provides 2 WO 6 The preparation method of glass-ceramics modification comprises the steps of: preparing graphene hybrid Bi 2 WO 6 Glass-ceramic powder to 0.5um size, using ultrasonic thermal spraying device to prepare graphene-containing hybrid Bi 2 WO 6 Glass-ceramic powder coating the surface of stainless steel wire for dynamic interception, mixing graphene with Bi 2 WO 6 The stainless steel wire used for dynamic interception of glass-ceramic glaze is placed in the dynamic interception device to realize Bi 2 WO 6 The self-cleaning and VOC degradation functions of the stainless steel wire used for the dynamic interception of the glass-ceramic glaze, this embodiment 2 makes full use of the oil fume to purify the heat energy and light energy of the stove itself, energy saving and environmental protection, one thing with multiple functions, and the process is simple.
[0032] In summary, in ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com