A high-adhesion, waterproof material technology, applied in the coating and other directions, can solve the problems of water accumulation in the bathroom, time-consuming and labor-intensive, poor adhesion, etc., to achieve good anti-cold and hot water effect, fast drying speed, and adhesion. strong effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] A high-adhesion waterproof material for smooth ground, comprising the following components in parts by weight: 25 parts of PVDC aqueous emulsion, 5 parts of nano-titanium oxide, 7 parts of itaconic acid, 10 parts of betaine, dihydrojasmonic acid A 5 parts of ester, 1 part of curing agent.
[0021] A preparation method of a high-adhesion waterproof material for smooth ground, comprising the following steps: (1) mixing PVDC aqueous emulsion, nano-titanium oxide and betaine, adding 40 parts of water, and stirring and mixing at room temperature for 1 hour; (2) ) respectively add itaconic acid and methyl dihydrojasmonate into the reactor for mixing, add an ethanol solution with a mass fraction of 85%, first place it at -35°C and stir for 1 hour, then heat it in a water bath and stir at 80°C React for 2 hours; (3) store the result of the previous step at -35°C for 10 hours; (4) then mix the result of step (1) with the result of step (3), and continue to stir and react at 78°C...
Embodiment 2
[0023] A high-adhesion waterproof material for smooth ground, comprising the following components in parts by weight: 40 parts of PVDC aqueous emulsion, 8 parts of nano-titanium oxide, 10 parts of itaconic acid, 15 parts of betaine, dihydrojasmonate methyl 8 parts of ester, 4 parts of curing agent.
[0024] A preparation method for a high-adhesion waterproof material for smooth ground, comprising the following steps: (1) mixing PVDC aqueous emulsion, nano-titanium oxide and betaine, adding 60 parts of water, and stirring and mixing at room temperature for 2 hours; (2) ) respectively add itaconic acid and methyl dihydrojasmonate into the reactor and mix them, add an ethanol solution with a mass fraction of 85%, first put it at -20°C and stir for 2 hours, then heat it in a water bath and stir at 95°C React for 4 hours; (3) store the result of the previous step at -20°C for 20 hours; (4) then mix the result of step (1) with the result of step (3), and continue to stir and react a...
Embodiment 3
[0026] A high-adhesion waterproof material for smooth ground, comprising the following components in parts by weight: 32 parts of PVDC aqueous emulsion, 7 parts of nano-titanium oxide, 8 parts of itaconic acid, 12 parts of betaine, dihydrojasmonic acid A 7 parts of ester, 2 parts of curing agent.
[0027] A method for preparing a high-adhesion waterproof material for smooth floors, comprising the following steps: (1) mixing PVDC aqueous emulsion, nano-titanium oxide and betaine, adding 45 parts of water, and stirring and mixing at room temperature for 1.6 hours. (2) Add itaconic acid and methyl dihydrojasmonate respectively into the reactor and mix them, add an ethanol solution with a mass fraction of 85%, first place it at -25°C for 1.3h, and then heat it in a water bath for 85 Stir the reaction at °C for 3 h; (3) Store the obtained product in the previous step at -30 °C for 16 h. (4) Then mix the product of step (1) with the product of step (3), and continue to stir and rea...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 