Magnetic adsorption material, preparation of magnetic adsorption material and method for treating thallium-containing wastewater
A magnetic adsorption material and waste water technology, applied in the direction of adsorption water/sewage treatment, chemical instruments and methods, water/sewage treatment, etc., can solve the high cost of thallium element material treatment, high input cost, unstable thallium removal effect, etc. question
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The magnetic adsorption material contains manganese ferrite and manganese dioxide, manganese dioxide (MnO 2 ) and manganese ferrite (MnFe 2 o 4 ) The mass ratio is 1:5.
[0019] The preparation method of the magnetic adsorption material is as follows: dissolve 12.10g (0.07mol) manganese acetate in 50ml distilled water, add 29.42g (0.14mol) citric acid to dissolve, add water to dilute to 100ml, adjust the pH value of the solution to 5.0~6.0 with ammonia water In between, add 30.45g manganese ferrite, stir evenly, ultrasonically treat for 30min to make it evenly mixed, spread it in a petri dish and put it in an oven to dry, grind it and roast it to get manganese dioxide loaded manganese ferrite, Save, spare, and make production records at the same time.
[0020] Wastewater sample 1: select desulfurization wastewater from the iron and steel industry with a thallium ion content of 950.0 μg / L and pH=6~7.
[0021] Experimental preparation: Add 10mg, 20mg, 30mg, 40mg and 5...
Embodiment 2
[0046] The magnetic adsorption material contains manganese ferrite and manganese dioxide, manganese dioxide (MnO 2 ) and manganese ferrite (MnFe 2 o 4 ) The mass ratio is 1:6.
[0047]The preparation method of the magnetic adsorption material is as follows: dissolve 12.10g (0.07mol) manganese acetate in 50ml distilled water, add 29.42g (0.14mol) citric acid to dissolve, add water to dilute to 100ml, adjust the pH value of the solution to 5.0~6.0 with ammonia water In between, add 36.54g manganese ferrite, stir evenly, ultrasonically treat for 30 minutes to make it evenly mixed, spread it in a petri dish and put it in an oven to dry, grind it and roast it to get manganese dioxide loaded manganese ferrite, Save, spare, and make production records at the same time.
[0048] For waste water sample 1: the treatment of waste water sample 3 with a magnetic adsorption material is the same as in Example 1.
[0049] The treated water was tested and the content of thallium ions was m...
PUM
![No PUM](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/noPUMSmall.5c5f49c7.png)
Abstract
Description
Claims
Application Information
![application no application](https://static-eureka.patsnap.com/ssr/23.2.0/_nuxt/application.06fe782c.png)
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com