Sphere-like graphene oxide and preparation method and application thereof
A graphene and spherical-like technology, which is applied in chemical instruments and methods, inorganic chemistry, carbon compounds, etc., can solve problems such as difficult separation, blockage and transportation, and fouling on the wall of the device, and achieve the effect of facilitating processing and transportation
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0028] The present invention relates to a kind of preparation method of spherical graphene oxide, comprises the following steps:
[0029] Spray-drying and assembling the graphene oxide material liquid obtained by uniformly dispersing the graphene oxide and the modifier to obtain the spherical-like graphene oxide;
[0030] The modifying agent is used to introduce C3-C8 hydrocarbon groups and / or substituted hydrocarbon groups, and optional aromatic groups and / or substituted aromatic groups;
[0031] In the graphene oxide feed liquid, the content of the graphene oxide is 0.05wt%-1wt%, and the content of the modifying agent is 0.03wt%-0.10wt%.
[0032] In the present invention, by controlling the number of carbon atoms of the modifier and controlling the ratio of graphene oxide and modifier, the modifier can have suitable density and length when the modifier is coupled to graphene oxide, and the molecular interaction between modifiers Moderate force can better adjust the shape of...
Embodiment 1
[0064] 1) Preparation of raw material graphene: get the graphene oxide dispersion prepared by the Hummers method, adjust the graphene oxide concentration to be 0.1wt% of the dispersion, add pentylamine to adjust its concentration to be 0.05wt% of the dispersion, ultrasonic dispersion;
[0065] 2) The modified graphene ultrafine powder is obtained through the spray drying step, the temperature is set at 210° C., the wind speed is adjusted, and the final output is 20 g / h (the wind speed is calibrated by the output).
Embodiment 2
[0067] 1) Preparation of raw graphene: get the graphene oxide dispersion prepared by the Hummers method, adjust the graphene oxide concentration to be 0.4wt% of the dispersion, add ethanolamine to adjust its concentration to be 0.05wt% of the dispersion, and ultrasonically dispersion;
[0068] 2) Through the spray drying step, the modified graphene ultrafine powder is obtained, the temperature is set at 190°C, the wind speed is adjusted, and the final output is 22g / h (the wind speed is calibrated by the output).