Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Preparation method of low-temperature-resistant imitation copper door coating

A low-temperature-resistant copper door technology, applied in polyester coatings, asphalt coatings, epoxy resin coatings, etc., can solve the problems of environmental protection, unfavorable daily maintenance of imitation copper doors, and affecting the effect of imitation copper

Active Publication Date: 2020-11-10
湖州菱创科技有限公司
View PDF4 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

This process directly causes the differences in the products of various enterprises, so this process is the most important, but at present, this process uses black-plated paint, which is neither environmentally friendly nor affects the effect of imitation copper, which is not conducive to the daily maintenance of imitation copper doors

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0018] A preparation method of a low-temperature-resistant imitation copper door coating, comprising the following steps:

[0019] A Add epoxy resin and carboxyl-terminated saturated polyester resin into the mixing tank, stir evenly at low speed;

[0020] B adds ethyl acetate and petroleum asphalt under the stirring condition of 420rpm;

[0021] C, add leveling agent and glycerol under 750rpm stirring condition and disperse evenly;

[0022] D Add iron oxide red and copper fine powder into the tank under 380rpm stirring condition;

[0023] E Add the remaining raw materials and stir evenly under the stirring condition of 1250rpm;

[0024] After F is ground, pass through a 250-mesh sieve, pack, and get final product.

[0025] The petroleum asphalt is liquid petroleum asphalt with a penetration of 0.1 mm (25° C.) of 110-130.

[0026] The leveling agent is an acrylate leveling agent.

[0027] The low-temperature-resistant imitation copper door coating is composed of the follow...

Embodiment 2

[0030] A preparation method of a low-temperature-resistant imitation copper door coating, comprising the following steps:

[0031] A Add epoxy resin and carboxyl-terminated saturated polyester resin into the mixing tank, stir evenly at low speed;

[0032] B adds ethyl acetate and petroleum asphalt under the stirring condition of 450rpm;

[0033] C, add leveling agent and glycerol under 600rpm stirring condition and disperse evenly;

[0034] D Add iron oxide red and copper fine powder into the tank under 450rpm stirring condition;

[0035] E Add the remaining raw materials and stir evenly under the stirring condition of 1200rpm;

[0036] After F is ground, pass through a 250-mesh sieve, pack, and get final product.

[0037] The petroleum asphalt is liquid petroleum asphalt with a penetration of 0.1 mm (25° C.) of 110-130.

[0038] The leveling agent is an acrylate leveling agent.

[0039] The low-temperature-resistant imitation copper door coating is composed of the follow...

Embodiment 3

[0042] A preparation method of a low-temperature-resistant imitation copper door coating, comprising the following steps:

[0043] A Add epoxy resin and carboxyl-terminated saturated polyester resin into the mixing tank, stir evenly at low speed;

[0044] B adds ethyl acetate and petroleum pitch under the stirring condition of 350rpm;

[0045] C, add leveling agent and glycerol under 800rpm stirring condition and disperse evenly;

[0046] D Add iron oxide red and copper fine powder into the tank under 350rpm stirring condition;

[0047] E Add the remaining raw materials and stir evenly under the stirring condition of 1500rpm;

[0048] After F is ground, pass through a 250-mesh sieve, pack, and get final product.

[0049] The petroleum asphalt is liquid petroleum asphalt with a penetration of 0.1 mm (25° C.) of 110-130.

[0050] The leveling agent is an acrylate leveling agent.

[0051] The low-temperature-resistant imitation copper door coating consists of the following c...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a preparation method of a low-temperature-resistant imitation copper door coating, which comprises the following steps: adding epoxy resin and carboxyl-terminated saturated polyester resin into a stirring cylinder, and uniformly stirring at low speed; adding ethyl acetate and petroleum asphalt under the stirring condition of 350-450rpm; adding leveling agent and glycerol under the condition of stirring at the speed of 600-800rpm, and uniformly dispersing; under the stirring condition of 350-450rpm, adding the iron oxide red and the copper fine powder into a cylinder forcolor matching; adding the rest raw materials, and uniformly stirring under the stirring condition of 1,200 to 1,500 rpm; and grinding, sieving with a 250-mesh sieve, and packaging. According to thelow-temperature-resistant imitation copper door coating, by adding the low-temperature-resistant glycerol and the organic bentonite with the interlayer structure, the low-temperature resistance of thecoating can be remarkably improved, and cracking is prevented; meanwhile, the iron oxide red, the liquid petroleum asphalt and the copper fine powder are mutually combined, so that the color mixing effect is better.

Description

technical field [0001] The invention relates to the technical field of copper imitation paint, in particular to a preparation method of a low temperature resistant copper imitation paint. Background technique [0002] The imitation copper door is made of electrolytic plates, and the surface is sprayed with paint with a color similar to that of the copper door to make it look similar to the copper door, so it is called an imitation copper door. In order to achieve a beautiful and durable effect, most of the domestic anti-theft doors are made of imitation copper doors, and most of them adopt pickling and phosphating process before painting. Plates, forgings and cold plates are welded together, which causes certain difficulties for spraying, so a primer for degreasing and rust removal is required in the early stage. First: Primer. At present, most enterprises use electrostatic powder spraying as primer. Second: finish paint, which is now basically in several colors of red cop...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09D163/00C09D167/00C09D195/00C09D7/61C09D7/63C09D7/62C09D7/47
CPCC09D163/00C09D7/61C09D7/63C09D7/62C09D7/47C08L2205/03C08K2003/2272C08L67/00C08L95/00C08K13/06C08K3/346C08K5/053C08K3/08C08K3/22
Inventor 姚晓祥
Owner 湖州菱创科技有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products