Preparation method of protective nano elastic insole
A technology of elasticity and insoles, which is applied in the field of preparation of protective nano-elastic insoles, can solve problems such as insufficient foot protection, and achieve the effect of mechanical improvement
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2021-02-26
Smart Images

Figure 1
Abstract
Description
technical field
[0001] The invention relates to a method for preparing protective nano-elastic insoles. Background technique
[0002] Special types of workers, such as hardware manufacturing, forestry, exploration and rescue operations, need to work in some special environments. Therefore, new designs need to be made for special safety protective shoes of special types of work. Due to the particularity of the occupation, such as military personnel, firefighters and other personnel, the load far exceeds that of ordinary people, and some lower limb injuries often occur, mainly manifested in excessive stretching of the arch ligament, calcaneal pain, forefoot pain and other symptoms. This is due to excessive peak pressure in the forefoot and heel area, resulting in severe compression of the nerves in the foot. In response to this situation, it is necessary to improve the protective insoles. There are many types of insoles used now, such as elastic foam materials EVA, TPU, clot...
Examples
Embodiment Construction
[0018] The preferred embodiments of the present invention will be described in detail below in conjunction with the accompanying drawings, so that the advantages and features of the present invention can be more easily understood by those skilled in the art, so as to define the protection scope of the present invention more clearly.
[0019] like figure 1 Shown is a kind of protective nano-elastic insole preparation method, comprises the steps:
[0020] S1, mastication: take natural rubber and put it into an open mill for mastication, and the temperature of the rollers of the open mill is 40-50°C;
[0021] S2, mixing: take a certain proportion of nitrile rubber and add it to the open mill to mix with natural rubber;
[0022] S3. Fragrance ratio: Take 20-40 parts of chlorhexidine hydrochloride powder, 16-20 parts of nano-silicon dioxide, 14-18 parts of zeolite powder, 24-30 parts of tourmaline powder, and 5-15 parts of chitosan powder to form a spice pink;
[0023] S4. Stirr...