Defoaming agent for landfill leachate and preparation method thereof
A technology of landfill leachate and defoaming agent, which is applied in separation methods, chemical instruments and methods, liquid degassing, etc., and can solve problems such as difficult and efficient defoaming of defoaming agents
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] This embodiment relates to a defoamer for landfill leachate, which includes the following components in parts by mass: 12 parts of modified abietic acid, 6 parts of fatty acid polyoxyethylene ester, 3 parts of alkaline silica sol, ethanol 1 part, 2 parts of isopropanol, 1.2 parts of emulsifier AEO-9, 1.2 parts of nonylphenol polyoxyethylene ether, 2.8 parts of PPG, the pH value of the alkaline silica sol is 9.5, and the silicon dioxide content is 30%, The average particle size is 8-20nm;
[0027] The preparation method of described defoamer is:
[0028] Weigh each raw material according to the stated mass parts for later use, first add the modified abietic acid and the ethanol and isopropanol into the reaction kettle, gradually heat up to dissolve, stir and mix for 30 minutes, keep the temperature and add the fatty acid polyoxygen Vinyl ester and the alkaline silica sol, continue to stir and mix for 30 minutes, add the emulsifier AEO-9, the nonylphenol polyoxyethylene ...
Embodiment 2
[0033]This embodiment relates to a defoamer for landfill leachate, which includes the following components in parts by mass: 12 parts of purified abietic acid, 6 parts of fatty acid polyoxyethylene ester, 3 parts of alkaline silica sol, 1 part of ethanol 2 parts, 2 parts of isopropanol, 1.2 parts of emulsifier AEO-9, 1.2 parts of nonylphenol polyoxyethylene ether, 2.8 parts of PPG, the pH value of the alkaline silica sol is 9.5, the silicon dioxide content is 30%, the average The particle size is 8-20nm;
[0034] The preparation method of described defoamer is:
[0035] Weigh each raw material according to the number of parts by mass for later use, first add the purified abietic acid and the ethanol and isopropanol into the reaction kettle, gradually heat up to dissolve, stir and mix for 30 minutes, and add the fatty acid polyoxyethylene ester and The alkaline silica sol was continuously stirred and mixed for 30 minutes, cooled to room temperature, added with the emulsifier A...
Embodiment 3
[0037] This embodiment relates to a defoamer for landfill leachate, which includes the following components in parts by mass: 12 parts of modified abietic acid, 6 parts of fatty acid polyoxyethylene ester, 3 parts of alkaline silica sol, ethanol 1 part, 2 parts of isopropanol, 1.2 parts of emulsifier AEO-9, 1.2 parts of nonylphenol polyoxyethylene ether, 2.8 parts of PPG, 0.8 parts of tert-butylphenyldiazosulfonate, the alkaline silica sol The pH value is 9.5, the silica content is 30%, and the average particle size is 8-20nm;
[0038] The preparation method of described defoamer is:
[0039] Weigh each raw material according to the stated mass parts for later use, first add the modified abietic acid and the ethanol and isopropanol into the reaction kettle, gradually heat up to dissolve, stir and mix for 30 minutes, keep the temperature and add the fatty acid polyoxygen Vinyl ester and the alkaline silica sol, continue to stir and mix for 30 minutes, add the emulsifier AEO-9,...
PUM
Property | Measurement | Unit |
---|---|---|
The average particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com