[0030] 1. Weigh 10 g of acid-activated montmorillonite, wash with 500 mL of deionized water, and centrifuge for 4 times. The pH of the wash water (that is, the cleaned deionized water) is 6.7. Then add 90 mL of deionized water and stir to prepare a slurry of montmorillonite suspension with a concentration of 10%.
[0031] 2. Weigh 1g of dodecyltrimethylammonium bromide and dissolve it in 100mL of deionized water to form a surfactant solution with a concentration of 1% by mass, and slowly pour into the above montmorillonite while stirring The suspension slurry was activated for 12 hours, during which stirring was continued, and then centrifuged for dehydration. After washing with deionized water for 4 times, add 190 mL of deionized water and stir to prepare activated montmorillonite suspension slurry with a concentration of 5%.
[0032] 3. Measure 5 mL of diethylenetriamine, slowly pour the above-mentioned activated montmorillonite suspension slurry while stirring, carry out the in...
Embodiment 2
[0036] 1. Weigh 10 g of acid-activated montmorillonite, wash with 500 mL of deionized water, and centrifuge for 5 times. The pH of the washing water (ie, cleaned deionized water) is 6.8. Then add 90 mL of deionized water and stir to prepare a montmorillonite suspension slurry with a concentration of 10%.
[0037] 2. Weigh 2g of dodecyltrimethylammonium bromide and dissolve it in 100mL of deionized water to form a surfactant solution with a concentration of 1% by mass, and slowly pour into the above montmorillonite while stirring The slurry was subjected to an activation reaction for 12 hours, during which stirring was continued, and then centrifuged for dehydration. After washing with deionized water for 4 times, add 190 mL of deionized water and stir to prepare activated montmorillonite suspension slurry with a concentration of 5%.
[0038] 3. Measure 5 mL of triethylenetetramine, slowly pour the above-mentioned activated montmorillonite suspension slurry while stirring, carry ou...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com