Coffee viscose fiber and preparation method thereof

A technology of viscose fiber and coffee, which is applied in the field of coffee viscose staple fiber and its production process, which can solve the problems of waste of resources and other problems, and achieve the effect of not easy to lose, comfortable hand feeling, antibacterial and deodorant function lasting

Active Publication Date: 2011-09-21
潍坊欣龙生物材料有限公司
View PDF4 Cites 17 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

A large number of residues are produced during the process of grinding and processing coffee, and the coffee grounds can absorb the peculi

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0016] Embodiment 1, coffee viscose fiber and preparation method thereof, comprises the following steps:

[0017] (1) Select cotton pulp for short silk production as the raw material, and go through the processes of impregnation, pressing, crushing, aging, yellowing, dissolution, defoaming, and filtration to obtain a viscose solution. The content of methylcellulose in the viscose solution is 8% ;

[0018] (2) Grind the coffee grounds into powder, grind the coffee grounds at 40-60°C for 2-4 hours with a spherical grinder, so that the particle size of the coffee grounds is below 2 microns, stir and disperse evenly in the aqueous solution to obtain a slurry, and put The slurry is evenly added to the viscose solution, fully stirred and mixed evenly to obtain a spinning viscose collagen solution, and the amount of coffee grounds added accounts for 10% of the weight of cellulose in the viscose solution;

[0019] (3) The prepared spinning viscose collagen solution is spun into a coa...

Embodiment 2

[0022] Embodiment 2, coffee viscose fiber and preparation method thereof, comprises the following steps:

[0023] (1) Select cotton pulp for short silk production as the raw material, and go through the processes of impregnation, pressing, crushing, aging, yellowing, dissolution, defoaming, and filtration to obtain a viscose solution. The content of methylcellulose in the viscose solution is 9% ;

[0024] (2) Grind the coffee grounds into powder with a particle size of less than 2 microns, uniformly disperse in the aqueous solution to obtain a slurry, uniformly add the slurry into the viscose solution, stir and mix well, and obtain a spinning viscose solution , the addition of coffee grounds accounts for 20% of the cellulose weight in the viscose solution;

[0025] (3) The prepared spinning viscose collagen solution is spun into a coagulation bath, and then the finished coffee viscose fiber is obtained through drafting, refining and drying processes. The coagulation bath is a...

Embodiment 3

[0028] Embodiment 3, coffee viscose fiber and preparation method thereof, comprises the following steps:

[0029] (1) Select cotton pulp for short silk production as the raw material, and go through the processes of impregnation, pressing, crushing, aging, yellowing, dissolution, defoaming, and filtration to obtain a viscose solution. The content of methylcellulose in the viscose solution is 10% ;

[0030] (2) Grind the coffee grounds into powder with a particle size of less than 2 microns, uniformly disperse in the aqueous solution to obtain a slurry, uniformly add the slurry into the viscose solution, stir and mix well, and obtain a spinning viscose solution , the addition of coffee grounds accounts for 30% of the cellulose weight in the viscose solution;

[0031] (3) The prepared spinning viscose collagen solution is spun into a coagulation bath, and then the finished coffee viscose fiber is obtained through drafting, refining and drying processes. The coagulation bath is ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
Dry breaking strengthaaaaaaaaaa
Dry breaking strengthaaaaaaaaaa
Dry breaking strengthaaaaaaaaaa
Login to view more

Abstract

The invention relates to coffee viscose fiber, which is prepared by crude materials including cotton pulp and coffee residue, wherein the content of the coffee residue accounts for 10 to 30 wt% of cellulose. A preparation method of the coffee viscose fiber comprises the following steps: taking pulp as a crude material for staple fiber production; performing processes including dipping, squeezing, crushing, aging, yellowing, dissolving, defoaming, and filtering so as to obtain a viscose solution; grinding coffee residue into powder and dispersing the powder into an aqueous solution to obtain a slurry; adding the slurry into the viscose solution to obtain a spinning viscose stock solution, wherein the addition amount of the coffee residue accounts for 10 to 30% by weight of the cellulose of the viscose solution; and carrying out spinning and molding on the prepared spinning viscose stock solution in a coagulating bath, and performing processes of drafting, refining, and drying to obtain a finished product of the coffee viscose fiber. According to the invention, the coffee residue, which is distributed evenly in the fiber, is not easy to be lost, so that the antibiotic and odor resistant functions of the coffee residue are lasting. The coffee viscose fiber not only has functions of bacteriostasis, deodorization, and moisture absorption and perspiration, but also has characteristics of moisture absorption and air permeability as well as comfortable wearing property of the viscose fiber. Textiles made from the coffee viscose fibers have a good moisture adsorption performance and a good moisture regain rate as well as have characteristics of comfortable hand feeling and softness and dryness.

Description

technical field [0001] The invention relates to a viscose fiber and a manufacturing method thereof, in particular to a coffee viscose staple fiber and a production process thereof. Background technique [0002] As a drink, coffee has gradually entered the life of modern people and is already a daily drink for many people. Coffee can improve heart function, dilate blood vessels, improve blood circulation, calm headaches, and refresh the mind. Coffee contains certain nutrients such as: vitamin B, free fatty acids, caffeine, tannic acid and so on. Coffee is good for the skin. Coffee can promote metabolism, activate digestive organs, and eliminate fatigue. In terms of health care, coffee has the functions of anti-oxidation and heart protection, strengthening muscles and bones, sharpening waist and knees, appetizing and promoting food, reducing fat and accumulation, benefiting orifices and dehumidification, promoting blood circulation and removing stasis, calming wind and reliev...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): D01F2/08D01D5/06
Inventor 曹其贵王乐军刘建华吴亚红姜明亮秦翠梅王东卢海蛟
Owner 潍坊欣龙生物材料有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products