An aerosol and water-based technology, which is applied in the field of water-based aerosol and its preparation, can solve problems such as no formula system found, environmental pollution, safety accidents, etc., and achieve large promotion profit margins, broad market prospects, and use safe effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] Sodium oleate 0.625g, fatty alcohol polyoxyethylene ether sodium sulfate 0.975g, sodium hydroxide 0.175g, sodium benzoate 0.08g, sodium nitrite 0.08g, deionized water 28.065g, and propane butane 10g.
[0021] Preparation method: Weigh the above-mentioned raw materials for use, add deionized water to the batching kettle, turn on the stirring, then add sodium hydroxide, sodium benzoate, and sodium nitrite in sequence, and stir for 8 minutes to completely dissolve them. Slowly add sodium oleate and fatty alcohol polyoxyethylene ether sodium sulfate, and continue to stir for 10 minutes to completely dissolve them. After passing the inspection, it is filtered with a 400-mesh filter and filled into the aerosol tank. After the valve is sealed, it is filled with propane and butane, and the spray cover is installed to obtain the finished product.
[0022] Table 1 shows the performance comparison between the water-based Feixue aerosol prepared in Example 1 and similar products in the ...
Embodiment 2
[0026] Nonylphenol polyoxyethylene ether 0.6g, sodium oleate 0.2g, sodium benzoate 0.12g, sodium nitrite 0.12g, deionized water 26.96g, and propanebutane 12g.
[0027] Preparation method: Weigh the above-mentioned raw materials for use, add deionized water to the batching kettle, turn on the stirring, and then add sodium benzoate and sodium nitrite in sequence, and stir for 6 minutes to completely dissolve them. Slowly add nonylphenol polyoxyethylene ether and sodium oleate and continue to stir for 15 minutes to completely dissolve them. After passing the inspection, it is filtered with a 300-mesh filter and filled into the aerosol tank. After the valve is sealed, it is filled with propane and butane, and the spray cap is installed to obtain the finished product.
Embodiment 3
[0029] Nonylphenol polyoxyethylene ether 3.2g, sodium benzoate 0.08g, sodium nitrite 0.08g, deionized water 30.64g, and propanebutane 6g.
[0030] Preparation method: Weigh the above-mentioned raw materials for use, add deionized water to the batching kettle, turn on the stirring, then add sodium benzoate and sodium nitrite in sequence, and stir for 10 minutes to completely dissolve them. Slowly add nonylphenol polyoxyethylene ether and continue to stir for 10 minutes to completely dissolve it. After passing the inspection, it is filtered with a 400-mesh filter and filled into the aerosol tank. After the valve is sealed, it is filled with propane and butane, and the spray cover is installed to obtain the finished product.
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com