Rubber gasket containing modified vermiculite nano-powder
A technology of rubber gaskets and vermiculite powder, applied in the field of rubber gaskets, can solve the problems of inconvenient production, service life and durability, high temperature resistance and weathering resistance, etc., and achieve long service life and good impact elasticity. , the effect of increasing the strength of the material
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0013] A rubber gasket containing modified nano-vermiculite powder, which is made of the following raw materials in parts by weight: 110 parts of fluororubber, 22 parts of polyvinyl chloride, 5 parts of dibenzothiazole disulfide, bismaleyl 8 parts of amine, 3.5 parts of dodecyl alcohol ester, 3 parts of glass fiber, 7 parts of modified nano vermiculite powder, 15 parts of asbestos, 13 parts of spray carbon black, 10 parts of coumarone, 6 parts of calcium carbonate, 6 parts of magnesium oxide 6 parts of calcium hydroxide, 7 parts of chlorinated paraffin, 2.2 parts of polyethylene wax, 5 parts of naphthenic oil, and 5 parts of modified tree ash.
[0014] Among them, the modified nano vermiculite powder is prepared by the following method: calcining the vermiculite at 700°C for 6 hours, then soaking it in a 10% sodium bicarbonate solution for 6 hours, drying it at 70°C, and grinding it into nano Powder is fine.
[0015] The modified tree ashes are prepared by the following metho...
Embodiment 2
[0018] A rubber gasket containing modified nano-vermiculite powder, which is made of the following raw materials in parts by weight: 120 parts of fluororubber, 27 parts of polyvinyl chloride, 7 parts of dibenzothiazole disulfide, bismaleyl 10 parts of amine, 3.4 parts of dodecyl alcohol ester, 4 parts of glass fiber, 6 parts of modified nano vermiculite powder, 18 parts of asbestos, 15 parts of spray carbon black, 12 parts of coumarone, 8 parts of calcium carbonate, 5 parts of magnesium oxide 6 parts of calcium hydroxide, 8 parts of chlorinated paraffin, 2.4 parts of polyethylene wax, 4 parts of naphthenic oil, and 6 parts of modified tree ash.
[0019] Wherein, the modified nano-vermiculite powder is prepared by the following method: calcining vermiculite at 800°C for 6 hours, then soaking in 11% sodium bicarbonate solution for 6 hours, drying at 80°C, It can be ground into nano powder.
[0020] The modified tree ashes are prepared by the following method: first soak the tre...
Embodiment 3
[0023] A rubber gasket containing modified nano-vermiculite powder, which is made of the following raw materials in parts by weight: 130 parts of fluororubber, 30 parts of polyvinyl chloride, 8 parts of dibenzothiazole disulfide, bismaleyl 2 parts of amine, 3.5 parts of dodecyl alcohol ester, 5 parts of glass fiber, 7 parts of modified nano vermiculite powder, 20 parts of asbestos, 16 parts of spray carbon black, 10 parts of coumarone, 10 parts of calcium carbonate, 5 parts of magnesium oxide 7 parts of calcium hydroxide, 9 parts of chlorinated paraffin, 2.5 parts of polyethylene wax, 5 parts of naphthenic oil, 7 parts of modified tree ash.
[0024] Wherein, the modified nano vermiculite powder is prepared by the following method: calcining the vermiculite at 900°C for 5 hours, then soaking it in a 12% sodium bicarbonate solution for 6 hours, drying it at 80°C, and drying it at 80°C. It can be ground into nano powder.
[0025] The modified tree ashes are prepared by the follo...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com