[0015] A kind of floor paint, its raw material proportioning by weight is as follows: 100 parts of modified alkyd resins; 10 parts of methyl methacrylates; 25 parts of calcium caprylates; 35 parts of xylenes; 55 parts of perfume; 5 parts of butyl acetate; 10 parts of red iron oxide; 1 part of azobisisobutyronitrile; 20 parts of dioxane; 15 parts of dimethylaminoethyl acrylate; 5 parts of dibutyl phthalate; 15 parts of nitrocellulose; 10 parts of zinc white; 30 parts of acetone.
[0016] Add acetone to pine water to dissolve, add iron oxide red, ochre, ball mill for 30 minutes with a ball mill, add dioxane, modified alkyd resin, methyl methacrylate, calcium octanoate, xylene and toluene, ball mill for 30 minutes, add Butyl acetate and the remaining raw materials were ball-milled for 1 hour and then filtered with gauze to obtain the finished product.
[0017] The product is 0.005g / cm2 in the reciprocating testing machine 1000 times 2 ; Adhesive strength 35MPa, no foaming and p...
Embodiment 2
[0019] A kind of floor paint, its raw material proportioning by weight is as follows: 100 parts of modified alkyd resins; 20 parts of methyl methacrylates; 35 parts of calcium caprylates; 45 parts of xylenes; 65 parts of perfume; 15 parts of butyl acetate; 20 parts of iron oxide red; 10 parts of azobisisobutyronitrile; 40 parts of dioxane; 25 parts of dimethylaminoethyl acrylate; 10 parts of dibutyl phthalate; 35 parts of nitrocellulose; 30 parts of zinc white; 40 parts of acetone.
[0020] Add acetone to pine water to dissolve, add iron oxide red, ochre, ball mill for 30 minutes with a ball mill, add dioxane, modified alkyd resin, methyl methacrylate, calcium octanoate, xylene and toluene, ball mill for 30 minutes, add Butyl acetate and the remaining raw materials were ball-milled for 1 hour and then filtered with gauze to obtain the finished product.
[0021] The product is 0.003g / cm2 in the reciprocating testing machine 1000 times 2 ; Bonding strength 40MPa, no foaming, n...
Embodiment 3
[0023] A kind of floor paint, its raw material proportioning by weight is as follows: 100 parts of modified alkyd resins; 15 parts of methyl methacrylates; 30 parts of calcium caprylates; 40 parts of xylenes; 60 parts of perfume; 10 parts of butyl acetate; 15 parts of red iron oxide; 5 parts of azobisisobutyronitrile; 30 parts of dioxane; 20 parts of dimethylaminoethyl acrylate; 8 parts of dibutyl phthalate; 25 parts of nitrocellulose; 20 parts of zinc white; 35 parts of acetone.
[0024] Add acetone to pine water to dissolve, add iron oxide red, ochre, ball mill for 30 minutes with a ball mill, add dioxane, modified alkyd resin, methyl methacrylate, calcium octanoate, xylene and toluene, ball mill for 30 minutes, add Butyl acetate and the remaining raw materials were ball-milled for 1 hour and then filtered with gauze to obtain the finished product.
[0025] The product is 0.001g / cm2 in the reciprocating testing machine 1000 times 2 ; Adhesive strength 45MPa, no foaming and...