Embodiment 1
[0030] An improved computer case shell is composed of two parts: a case body and an antibacterial heat dissipation ceramic, and the parts by weight of the raw material components of the antibacterial heat dissipation ceramic coating are:
[0031]
[0032] An antibacterial heat dissipation ceramic coating processing method for an improved computer case shell, which comprises the following steps:
[0033] (1): Preparation of functional polysiloxane prepolymer: select nano-silicon nitride with a particle size of 60nm, use a mixed solvent of deionized water and alcohol for ultrasonic dispersion, and the ultrasonic dispersion time is 30min, the volume of water and alcohol The ratio is 1:1, the alcohol is isopropanol, and the mass concentration of nano-silicon nitride in the mixed solvent is 0.1 g / L. After the dispersion is complete, add a nitric acid catalyst to the dispersion to adjust the pH of the system to 2, then add a mixture of methyltrialkoxysilane and vinyltrialkoxysila...
Embodiment 2
[0038] An improved computer case shell is composed of two parts: a case body and an antibacterial heat dissipation ceramic, and the parts by weight of the raw material components of the antibacterial heat dissipation ceramic coating are:
[0039]
[0040] An antibacterial heat dissipation ceramic coating processing method for an improved computer case shell, which comprises the following steps:
[0041] (1): Preparation of functional polysiloxane prepolymer: select nano-silicon nitride with a particle size of 80nm, use a mixed solvent of deionized water and alcohol for ultrasonic dispersion, and the ultrasonic dispersion time is 45min, the volume of water and alcohol The ratio is 1:5, the alcohol is ethanol, and the mass concentration of nano-silicon nitride in the mixed solvent is 2.5g / L. After the dispersion is complete, add a nitric acid catalyst to the dispersion to adjust the pH of the system to 4, then add a mixture of methyltrialkoxysilane and vinyltrialkoxysilane, a...
Embodiment 3
[0046] An improved computer case shell is composed of two parts: a case body and an antibacterial heat dissipation ceramic, and the parts by weight of the raw material components of the antibacterial heat dissipation ceramic coating are:
[0047]
[0048] An antibacterial heat dissipation ceramic coating processing method for an improved computer case shell, which comprises the following steps:
[0049](1): Preparation of functional polysiloxane prepolymer: Select nano-silicon nitride with a particle size of 60nm, use a mixed solvent of deionized water and alcohol for ultrasonic dispersion, and the ultrasonic dispersion time is 35min, the volume of water and alcohol The ratio is 1:2.5, the alcohol is isopropanol, and the mass concentration of nano-silicon nitride in the mixed solvent is 1.0 g / L. After the dispersion is complete, add a nitric acid catalyst to the dispersion to adjust the pH of the system to 3, then add a mixture of methyltrialkoxysilane and vinyltrialkoxysil...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com