Embodiment 1
[0043] The preparation method of the environment-friendly water-based metallic ink of the present embodiment, it comprises the following preparation steps:
[0044] a. Add 20 parts of modified water-based acrylic resin, 40 parts of modified water-based polyurethane, 14 parts of deionized water, and 2 parts of industrial ethanol into the batching tank and stir evenly;
[0045] b. Add 10 parts of dispersant, 0.5 parts of defoamer and 20 parts of silver powder to the material mixed in step a and stir evenly for 20 minutes;
[0046] c. Stir 0.5 part of surfactant, 1 part of adhesion promoter and the materials mixed in step b evenly, and ultrasonically vibrate for 30 minutes to prepare an environment-friendly water-based metal ink.
Embodiment 2
[0048] The preparation method of the environment-friendly water-based metallic ink of the present embodiment, it comprises the following preparation steps:
[0049] a. Add 15 parts of modified water-based acrylic resin, 30 parts of modified water-based polyurethane, 12 parts of deionized water, and 3 parts of industrial ethanol into the batching tank and stir evenly;
[0050] b. Add 9 parts of dispersant, 0.8 parts of defoamer and 16 parts of copper powder to the material mixed in step a and stir evenly, and the stirring time is 22 minutes;
[0051] c. Stir 1.2 parts of surfactant, 5 parts of adhesion promoter and the materials mixed in step b evenly, and ultrasonically vibrate for 28 minutes to prepare an environment-friendly water-based metal ink.
Embodiment 3
[0053] The preparation method of the environment-friendly water-based metallic ink of the present embodiment, it comprises the following preparation steps:
[0054]a. Add 20 parts of modified water-based acrylic resin, 20 parts of modified water-based polyurethane, 11 parts of deionized water, and 4 parts of industrial ethanol into the batching tank and stir evenly;
[0055] b. Add 8 parts of dispersant, 1 part of defoamer and 10 parts of gold powder to the material mixed in step a and stir evenly. The stirring time is 24 minutes;
[0056] c. Stir 5 parts of surfactant, 4 parts of adhesion promoter and the materials mixed in step b evenly, and ultrasonically vibrate for 26 minutes to prepare an environment-friendly water-based metal ink.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com