A polyvinyl chloride and pipe technology, applied in the direction of pipes, rigid pipes, mechanical equipment, etc., can solve the problems of low ring stiffness, poor antibacterial performance of polyvinyl chloride, limited application scope, etc., and achieve aging resistance and thermal stability. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] An antibacterial reinforced polyvinyl chloride pipe, the components of which are proportioned by mass percentage: 45% polyvinyl chloride, 12% carbon nanofiber, 10% dioctyl phthalate, 10% attapulgite, and 9% nitrile rubber , methacrylate-acrylate copolymer 6%, silver ion calcium phosphate 3%, light stabilizer UV-326 2%, calcium zinc composite stabilizer 1.5%, calcium stearate 1%, antioxidant 1010 0.5% , the carbon nanofibers are vapor-grown carbon nanofibers with a diameter of 50nm to 200nm and a surface modified by O2 plasma; nano-scale attapulgite.
[0018] Preparation method: (1), put the vapor-grown carbon nanofibers with a diameter of 50nm to 200nm in an O2 plasma box with a vacuum degree of 1 to 0.2mmHg and an input voltage of 220V, and treat them for 1 to 3 minutes, then dry them in dry air (2) Weigh each component according to the weight ratio, including the carbon nanofiber obtained in step (1); (3) mix polyvinyl chloride, o-phthalic Add dioctyl dicarboxylate ...
Embodiment 2
[0020] An antibacterial reinforced polyvinyl chloride pipe, the components of which are: 70% polyvinyl chloride, 8% nano-carbon fiber, 5% dioctyl phthalate, 5% attapulgite, and 6% nitrile rubber , Methacrylate-acrylate copolymer 3%, silver ion antibacterial zeolite 1%, light stabilizer UV-326 0.5%, calcium zinc composite stabilizer 0.5%, calcium stearate 0.8%, antioxidant 1010 0.2% , the carbon nanofibers are vapor-grown carbon nanofibers with a diameter of 50nm to 200nm and a surface modified by O2 plasma; nano-scale attapulgite.
[0021] Preparation method: (1), put the vapor-grown carbon nanofibers with a diameter of 50nm to 200nm in an O2 plasma box with a vacuum degree of 1 to 0.2mmHg and an input voltage of 220V, and treat them for 1 to 3 minutes, then dry them in dry air (2) Weigh each component according to the weight ratio, including the carbon nanofiber obtained in step (1); (3) mix polyvinyl chloride, o-phthalic Add dioctyl dicarboxylate and calcium-zinc composite...
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Particle size | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com