Looking for breakthrough ideas for innovation challenges? Try Patsnap Eureka!

Gold ore low-toxicity efficient mineral separation addition agent and preparing method thereof

A technology of auxiliary agent and gold ore, which is applied in the field of low-toxicity, high-efficiency beneficiation auxiliary agent and its preparation field of gold ore to achieve the effect of improving chemical properties, reducing dosage and strong oxidizing property.

Active Publication Date: 2016-04-06
GUANGXI SENHE HIGH TECH CO LTD
View PDF4 Cites 7 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] Aiming at the problems existing in the existing cyanidation process gold ore beneficiation agent, the present invention provides a low-toxicity and high-efficiency ore beneficiation aid for gold ore and its preparation method

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0021] A low-toxicity and high-efficiency mineral processing aid for gold mines, consisting of the following raw materials in parts by weight: 40 parts of thiourea, 25 parts of potassium ferrocyanide, 10 parts of sodium tripolyphosphate, 10 parts of ammonium iodide, and 10 parts of ammonium persulfate 10 parts of sodium peroxide, 20 parts of sodium carbonate, 8 parts of sodium hydroxide and 4 parts of sodium dodecylsulfonate.

[0022] Preparation method: Weigh 40 parts of raw materials thiourea, 25 parts of potassium ferrocyanide, 10 parts of sodium tripolyphosphate, 10 parts of ammonium iodide, 10 parts of ammonium persulfate, 10 parts of sodium peroxide, and 20 parts of sodium carbonate according to the proportioning ratio. Parts, 8 parts of sodium hydroxide, the raw materials were added into the mixer and mixed evenly to obtain the mixed material, then the mixed material was added to the reactor and heated to 700 ° C, kept for 2 hours, cooled to normal temperature to obtain ...

Embodiment 2

[0024] A low-toxic, high-efficiency mineral processing aid for gold mines, consisting of the following raw materials in parts by weight: 45 parts of thiourea, 20 parts of potassium ferrocyanide, 12 parts of sodium tripolyphosphate, 8 parts of ammonium iodide, and 12 parts of ammonium persulfate parts, 8 parts of sodium peroxide, 25 parts of sodium carbonate, 6 parts of sodium hydroxide and 5 parts of sodium dodecylsulfonate.

[0025] Preparation method: Weigh 45 parts of raw materials thiourea, 20 parts of potassium ferrocyanide, 12 parts of sodium tripolyphosphate, 8 parts of ammonium iodide, 12 parts of ammonium persulfate, 8 parts of sodium peroxide, and 25 parts of sodium carbonate according to the proportioning ratio. 1 part, 6 parts of sodium hydroxide, respectively put the raw materials into the mixer and mix evenly to obtain the mixed material, then put the mixed material into the reactor and heat it to 750°C, keep it warm for 1.5h, and cool to normal temperature to obt...

Embodiment 3

[0027] A low-toxicity and high-efficiency mineral processing aid for gold mines, consisting of the following raw materials in parts by weight: 50 parts of thiourea, 35 parts of potassium ferrocyanide, 12 parts of sodium tripolyphosphate, 12 parts of ammonium iodide, and 12 parts of ammonium persulfate 10 parts of sodium peroxide, 30 parts of sodium carbonate, 8 parts of sodium hydroxide and 6 parts of sodium dodecylsulfonate.

[0028] Preparation method: Weigh 50 parts of thiourea, 35 parts of potassium ferrocyanide, 12 parts of sodium tripolyphosphate, 12 parts of ammonium iodide, 12 parts of ammonium persulfate, 10 parts of sodium peroxide, and 30 parts of sodium carbonate according to the ratio of raw materials. Parts, 10 parts of sodium hydroxide, and respectively added to the mixer and mixed uniformly to obtain a mixed material, then the mixed material was added to the reactor and heated to 750 ° C, kept for 2 hours, cooled to normal temperature, to obtain the reaction pro...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a gold ore low-toxicity efficient mineral separation addition agent and a preparing method of the agent. The gold ore low-toxicity efficient mineral separation addition agent comprises, by weight, 40 parts to 60 parts of thiourea, 20 parts to 40 parts of potassium ferrocyanide, 10 parts to 15 parts of sodium tripolyphosphate, 8 parts to 15 parts of ammonium iodide, 10 parts to 15 parts of ammonium persulfate, 8 parts to 12 parts of sodium peroxide, 20 parts to 40 parts of sodium carbonate, 5 parts to 10 parts of sodium hydroxide and 4 parts to 8 parts of sodium dodecyl sulfate. The gold ore low-toxicity efficient mineral separation addition agent has the advantages of being low in toxicity, environment-friendly, low in production cost, simple in preparing technology, high in gold recycling rate, wide in raw material source and the like, and has the good social benefits, the ecological benefits and the economic benefits.

Description

technical field [0001] The invention relates to a precious metal beneficiation agent, in particular to a gold ore beneficiation aid with low toxicity and high efficiency and a preparation method thereof. Background technique [0002] With the continuous improvement of people's living standards, the demand for gold is rapidly expanding. Only by constantly looking for, developing and utilizing new gold mineral resources can the needs of today's society be met. The existing gold ore beneficiation methods mainly include flotation, gravity separation, cyanidation and so on. More than 85% of the gold in the world is extracted by cyanidation, which is a relatively mature process for extracting gold. The cyanidation method has the advantages of high recovery rate of gold extraction, strong adaptability to ore, simple method, on-site gold production, and low cost. However, the cyanidation method has the following disadvantages: cyanide is highly toxic, causing serious harm to the e...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C22B11/08
Inventor 阙明
Owner GUANGXI SENHE HIGH TECH CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products