Anti-static thermal-insulating adhesive
An anti-static and heat-insulating technology, applied in the direction of adhesives, adhesive types, adhesive additives, etc., can solve problems such as single function, and achieve the effect of wide application, good use effect and simple production.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0008] 24 parts of lithium silicate, 20 parts of graphite balls, 16 parts of vanadium trioxide, 10 parts of azodicarbonamide, 8 parts of zinc oxide, 4 parts of benzoyl peroxide, 10 parts of polyurethane, 40 parts of silicone, polyamide 20 parts of imine, 40 parts of polyisobutyl ester, 40 parts of phenolic resin, 10 parts of magnesium silicate, 20 parts of acetone, 10 parts of benzoyl peroxide, 10 parts of azodicarbonamide, 20 parts of benzoyl peroxide, Put 10 parts of dibutyl phthalate and 12 parts of triphenyl phosphate into the reactor, stir continuously, heat to 50°C after mixing completely, and get the product after uniform stirring.
Embodiment 2
[0010] 30 parts of lithium silicate, 25 parts of graphite balls, 17 parts of vanadium trioxide, 15 parts of azodicarbonamide, 10 parts of zinc oxide, 8 parts of benzoyl peroxide, 15 parts of polyurethane, 50 parts of silicone, polyamide 40 parts of imine, 50 parts of polyisobutyl ester, 60 parts of phenolic resin, 15 parts of magnesium silicate, 25 parts of acetone, 11 parts of benzoyl peroxide, 15 parts of azodicarbonamide, 25 parts of benzoyl peroxide, Put 11 parts of dibutyl phthalate and 16 parts of triphenyl phosphate into the reactor, stir continuously, heat to 50°C after mixing completely, and get the product after uniform stirring.
Embodiment 3
[0012] 36 parts of lithium silicate, 30 parts of graphite balls, 18 parts of vanadium trioxide, 20 parts of azodicarbonamide, 12 parts of zinc oxide, 12 parts of benzoyl peroxide, 20 parts of polyurethane, 60 parts of silicone, polyamide 60 parts of imine, 60 parts of polyisobutyl ester, 80 parts of phenolic resin, 20 parts of magnesium silicate, 30 parts of acetone, 12 parts of benzoyl peroxide, 20 parts of azodicarbonamide, 30 parts of benzoyl peroxide, Put 12 parts of dibutyl phthalate and 20 parts of triphenyl phosphate into the reactor, stir continuously, heat to 50°C after mixing completely, and get the product after uniform stirring.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com