An ammonia nitrogen removal rate, river water technology, applied in chemical instruments and methods, water pollutants, water/sewage treatment, etc., can solve problems such as unsuitable use, low ammonia nitrogen rate in biological floating beds, large investment and operating costs, and achieve no equipment. Maintenance cost, high nitrification rate, fast effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Select natural clinoptilolite ore, crush and pass through a 0.1mm sieve to obtain natural zeolite powder; mix aluminum powder, lime and surfactant in a mass ratio of 1:80:10 to obtain a foaming agent; in a mass ratio of 100:20: 1.5 Mix natural zeolite powder, cement and foaming agent to obtain a mixture; pour the mixture into a shape for initial setting for 1 to 2 hours, and cut it into blocks (length: 600mm, The width is 100mm, 125mm, 150mm, 200mm, 250mm, 300mm, 120mm, 180mm, 240mm and other specifications, and the height is 200mm, 250mm, 300mm and other specifications), and then put into the autoclaved curing kettle under 12Mpa pressure and steam at 180℃ Curing for 15 hours to obtain zeolite aerated concrete blocks.
[0016] Construction of infiltration dams for river trenches using zeolite air-entrained concrete blocks. The height of the seepage dam is 30cm higher than the normal water level of the ditch, and the length of the seepage dam is equal to the width of th...
Embodiment 2
[0019] Select natural clinoptilolite ore, crush and pass through a 0.1mm sieve to obtain natural zeolite powder; mix aluminum powder, lime and surfactant in a mass ratio of 1:50:5 to obtain a foaming agent; in a mass ratio of 20:4: 1. Mix natural zeolite powder, cement and foaming agent to obtain a mixture; pour the mixture into shape and initially set for 1 to 2 hours, and cut it into blocks (600mm in length) with a wire cutter from three directions: vertical, horizontal and horizontal , the width is 100mm, 125mm, 150mm, 200mm, 250mm, 300mm, 120mm, 180mm, 240mm and other specifications, the height is 200mm, 250mm, 300mm and other specifications), and then put into the autoclaved curing kettle under 12Mpa pressure and 180℃ temperature Steam curing for 15 hours to obtain zeolite aerated concrete blocks.
[0020] Use zeolite aerated concrete blocks to build drainage ditches with a width of 50-100 cm and a depth equal to twice the height of the blocks. Drainage flows through the...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com