Production method of mirror-surface metal leatherette paper
A production method and mirror metal technology, which are applied in chemical instruments and methods, papermaking, packaging paper, etc., can solve the problems of not many reports on the production process of mirror metal filled vellum paper, and the performance of mirror metal filled vellum paper is not very good, so as to achieve a good hand feeling. , Improve the effect of anti-mildew and anti-corrosion, and improve water resistance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The production method of a kind of mirror metal leather-filled paper proposed by the present invention comprises the selection of the original leather-filled backing paper, dipping processing, finishing, primer coating, compounding and embossing; the primer coating adopts the method of comma scraper coating, Apply the primer coating evenly on the finished paper surface, the primer coating amount is 30g / m 2 , the drying temperature is 110°C, and the vehicle speed is 30m / min.
Embodiment 2
[0020] The production method of a kind of mirror metal leather-filled paper proposed by the present invention comprises the selection of the original leather-filled backing paper, dipping processing, finishing, primer coating, compounding and embossing; the primer coating adopts the method of comma scraper coating, Apply the primer coating evenly on the finished paper surface, the primer coating amount is 15g / m 2 , the drying temperature is 130°C, and the vehicle speed is 20m / min.
Embodiment 3
[0022] The production method of a kind of mirror metal leather-filled paper proposed by the present invention comprises the selection of the original leather-filled backing paper, dipping processing, finishing, primer coating, compounding and embossing; the primer coating adopts the method of comma scraper coating, Apply the primer coating evenly on the finished paper surface, the primer coating amount is 17g / m 2 , the drying temperature is 125°C, and the vehicle speed is 24m / min;
[0023] Wherein, the primer coating is waterborne polyurethane resin;
[0024] The raw materials of the waterborne polyurethane resin include by weight: 30 parts of polyurethane prepolymer, 10 parts of butyl acetate, 30 parts of water, 3 parts of vinyltrimethoxysilane, 1 part of carbon black, 1 part of nano-titanium dioxide, talcum powder 0.2 parts, 1.5 parts of precipitated barium sulfate, 0.2 parts of organic bentonite, 2 parts of ethylene bisstearamide, 1 part of neopentyl glycol, 1.5 parts of 1...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com