A method for hydrochloric acid decomposition of phosphorus tailings to produce magnesium hydroxide and calcium sulfate
A technology of magnesium hydroxide and phosphorus tailings, which is applied in the directions of magnesium hydroxide, calcium/strontium/barium sulfate, ammonium salt fertilizers, etc., can solve the problems of overcapacity, low quality, restricting the production capacity of compound fertilizers, etc., and achieve production costs. Low cost, simple production process, and the effect of reducing environmental pressure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Phosphorus tailings and water are made into a slurry at a mass ratio of 1:0.5, and hydrochloric acid is added to the leaching tank to fully mix and react. The ratio of the molar amount of hydrochloric acid to the sum of the molar amounts of CaO and MgO in the phosphorous tailings is 1.6:1 , control the reaction temperature at 30°C, react for 0.5h under the condition of sufficient stirring, filter and separate to obtain slag I and mother liquor I, add sulfuric acid with a molar ratio of CaO of 1:1 to the mother liquor I to react and crystallize, and then enter the filtration and separation. Wash the filter cake with water to obtain the product calcium sulfate whiskers and mother liquor II, add ammonia water to the mother liquor II for two-stage neutralization, one-stage neutralization to control the pH to 2.5, filter and separate slag II and mother liquor III, and perform two-stage neutralization for mother liquor III , control the pH to 6.5, filter and separate to obtain...
Embodiment 2
[0035] Phosphorus tailings and water are made into a slurry at a mass ratio of 1:0.7, and hydrochloric acid is added to the leaching tank to fully mix and react. The ratio of the molar amount of hydrochloric acid to the sum of the molar amounts of CaO and MgO in the phosphorous tailings is 1.8:1 , control the reaction temperature at 30°C, react for 0.5h under the condition of sufficient stirring, filter and separate to obtain slag I and mother liquor I, add sulfuric acid with a molar ratio of CaO of 1:1 to the mother liquor I to react and crystallize, and then enter the filtration and separation. Wash the filter cake with water to obtain the product calcium sulfate whiskers and mother liquor II, add ammonia water to the mother liquor II for two-stage neutralization, one-stage neutralization to control the pH to 3.0, filter and separate slag II and mother liquor III, and carry out two-stage neutralization for mother liquor III , control the pH to 7.0, filter and separate to obta...
Embodiment 3
[0038] Phosphorus tailings and water are made into a slurry at a mass ratio of 1:0.8, and hydrochloric acid is added to the leaching tank to fully mix and react. The ratio of the molar amount of hydrochloric acid to the sum of the molar amounts of CaO and MgO in the phosphorous tailings is 1.7:1 , control the reaction temperature at 30°C, react for 0.5h under the condition of sufficient stirring, filter and separate to obtain slag I and mother liquor I, add sulfuric acid with a molar ratio of CaO of 1:1 to the mother liquor I to react and crystallize, and then enter the filtration and separation. Wash the filter cake with water to obtain the product calcium sulfate whiskers and mother liquor II, add ammonia water to the mother liquor II for two-stage neutralization, one-stage neutralization to control the pH to 3.0, filter and separate slag II and mother liquor III, and carry out two-stage neutralization for mother liquor III , control the pH to be 7.5, filter and separate to o...