Tungsten alloy shielding plate and electronic information card provided with tungsten alloy shielding plate
An electronic information card and tungsten alloy technology, applied in the field of electronic information cards, can solve problems such as illegal reading of magnetic track information, bank card information leakage, cardholder fund theft, etc., to prevent illegal reading or interference, thin thickness , Avoid the effect of funds being stolen
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] The tungsten alloy shielding plate in this embodiment includes components by mass percentage: 90% tungsten, 6% nickel, 3% copper, 0.5% cobalt, and 0.5% rare earth. Among them, tungsten, nickel, copper, and cobalt are respectively tungsten powder, nickel powder, copper powder, and cobalt powder.
[0019] The preparation method of the above-mentioned tungsten alloy shielding plate is as follows: in terms of mass percentage, pour 90% tungsten, 6% nickel, 3% copper, 0.5% cobalt, and 0.5% rare earth into the container, and then place it in a vacuum heating furnace for drying treatment , the drying temperature was 75°C, the vacuum degree was 5 Pa, and the drying time was 30 minutes to obtain a dry powder; the prepared dry powder was mixed in a ball mill for 10 hours to obtain a mixed powder; the prepared mixed powder was poured into In the compression mold, flatten, perform compression molding treatment, demould, and obtain a tungsten alloy powder metallurgy green body; put t...
Embodiment 2
[0028] The tungsten alloy shielding plate in this embodiment includes components by mass percentage: 94% tungsten, 3% nickel, 2% copper, 0.5% cobalt, and 0.5% rare earth. Among them, tungsten, nickel, copper, and cobalt are respectively tungsten powder, nickel powder, copper powder, and cobalt powder.
[0029] The preparation method of the above-mentioned tungsten alloy shielding plate is: in terms of mass percentage, pour 94% tungsten, 3% nickel, 2% copper, 0.5% cobalt, and 0.5% rare earth into a container, and then place it in a vacuum heating furnace for drying treatment , the drying temperature was 75°C, the vacuum degree was 5 Pa, and the drying time was 30 minutes to obtain a dry powder; the prepared dry powder was mixed in a ball mill for 10 hours to obtain a mixed powder; the prepared mixed powder was poured into In the compression mold, flatten, perform compression molding treatment, demould, and obtain a tungsten alloy powder metallurgy green body; put the prepared g...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com